MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dioshy TPU T990M Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Can be classified into two types of TPU with different soft segment compositions; ester group or ether group.

Features:

  • DIOSHY® TPE- TPU Series, well processing abilities, tough and elastic; suitable to abrasion resistance, oil resistance and mechanical properties needed.
  • Transparent and neutral color with good coloring ability. Can be customized to transparent or even super transparent.
  • Suitable to mostly thermoplastic procedures, PVC replacement, soft and flexible artificial leather.
  • Green material, passed heavy metal regulation, RoHS and EACH – SVHC .

      Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccJIS-K7311
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90JIS-K7311
Tensile Strength 400 kg(f)/cm²JIS-K7311
Elongation at Break 600 %JIS-K7311
100% Modulus 100 kg(f)/cm²JIS-K7311
Rebound 45 %
@Temperature 70.0 °C
resilience; JIS-K7311
Abrasion 35[mg], Taber; JIS-K7311
Compression Set 32 %
@Temperature 70.0 °C,
Time 79200 sec
JIS-K6301
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 118 °CJIS-K7206
Glass Transition Temp, Tg -43.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 155 - 165 °CInjection
 155 - 175 °CExtrusion
Middle Barrel Temperature 170 - 185 °CExtrusion
 175 - 185 °CInjection
Front Barrel Temperature 175 - 185 °CInjection
 175 - 190 °CExtrusion
Nozzle Temperature 195 - 205 °CInjection
Die Temperature 180 - 195 °CExtrusion
Drying Temperature 90.0 °C
Dry Time 3.00 hour
 
Descriptive Properties
Polyol typePolyester
TransparenceStandard

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDIOSH060 / 294670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.