MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dioshy TPU T990M Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Can be classified into two types of TPU with different soft segment compositions; ester group or ether group.

Features:

  • DIOSHY® TPE- TPU Series, well processing abilities, tough and elastic; suitable to abrasion resistance, oil resistance and mechanical properties needed.
  • Transparent and neutral color with good coloring ability. Can be customized to transparent or even super transparent.
  • Suitable to mostly thermoplastic procedures, PVC replacement, soft and flexible artificial leather.
  • Green material, passed heavy metal regulation, RoHS and EACH – SVHC .

      Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccJIS-K7311
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090JIS-K7311
Tensile Strength 39.2 MPa5690 psiJIS-K7311
Elongation at Break 600 %600 %JIS-K7311
100% Modulus 9.81 MPa1420 psiJIS-K7311
Rebound 45 %
@Temperature 70.0 °C
45 %
@Temperature 158 °F
resilience; JIS-K7311
Abrasion 3535[mg], Taber; JIS-K7311
Compression Set 32 %
@Temperature 70.0 °C,
Time 79200 sec
32 %
@Temperature 158 °F,
Time 22.0 hour
JIS-K6301
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 118 °C244 °FJIS-K7206
Glass Transition Temp, Tg -43.0 °C-45.4 °FDSC
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 155 - 165 °C311 - 329 °FInjection
 155 - 175 °C311 - 347 °FExtrusion
Middle Barrel Temperature 170 - 185 °C338 - 365 °FExtrusion
 175 - 185 °C347 - 365 °FInjection
Front Barrel Temperature 175 - 185 °C347 - 365 °FInjection
 175 - 190 °C347 - 374 °FExtrusion
Nozzle Temperature 195 - 205 °C383 - 401 °FInjection
Die Temperature 180 - 195 °C356 - 383 °FExtrusion
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
Polyol typePolyester
TransparenceStandard

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDIOSH060 / 294670

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.