MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Hot Work Steel

Material Notes: W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to optimized production techniques including the use of Vacuum Arc Remelting, and improved diffusion annealing and structurally treatments. These changes have led to a high degree of cleanliness, of uniformity of cleanliness, toughness and dimensional stability.

Use this grade where an improved version of W303 is required. Applications include highly stressed hot work tools, such as mandrels, dies and containers for metal tube and rod extrusion; hot extrusion tools; tools for the manufacture of hollows: tools for the manufacture of screws, nuts, rivets and bolts; forging dies and punches; die casting dies; forming dies; or hot shear blades.

Key Words: EN/DIN 1.2367, X38CrMoV5-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.65 g/cc
@Temperature 600 °C
 7.69 g/cc
@Temperature 500 °C
 7.85 g/cc
@Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 205as delivered
Hardness, Rockwell C 55hardened 1025°C then tempered 500°C
Modulus of Elasticity 165 GPa
@Temperature 600 °C
 176 GPa
@Temperature 500 °C
 215 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000500 ohm-cm
@Temperature 20.0 °C
 0.0000860 ohm-cm
@Temperature 500 °C
 0.0000960 ohm-cm
@Temperature 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 - 100 °C
 12.0 µm/m-°C
@Temperature 20.0 - 200 °C
 12.2 µm/m-°C
@Temperature 20.0 - 300 °C
 12.5 µm/m-°C
@Temperature 20.0 - 400 °C
 12.9 µm/m-°C
@Temperature 20.0 - 500 °C
 13.0 µm/m-°C
@Temperature 20.0 - 600 °C
 13.2 µm/m-°C
@Temperature 20.0 - 700 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.550 J/g-°C
@Temperature 500 °C
 0.590 J/g-°C
@Temperature 600 °C
Thermal Conductivity 28.4 W/m-K
@Temperature 100 °C
 29.7 W/m-K
@Temperature 200 °C
 29.7 W/m-K
@Temperature 600 °C
 30.0 W/m-K
@Temperature 700 °C
 30.0 W/m-K
@Temperature 500 °C
 30.1 W/m-K
@Temperature 400 °C
 30.2 W/m-K
@Temperature 300 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.38 %
Chromium, Cr 5.0 %
Iron, Fe 90.7 %As Balance
Manganese, Mn 0.25 %
Molybdenum, Mo 2.8 %
Silicon, Si 0.20 %
Vanadium, V 0.65 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm BÖHLER W303 ISODISC® Hot Work Tool Steel
Bohler-Uddeholm UDDEHOLM DIEVAR® Hot Work Tool Steel
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
Latrobe LSS™ 2367 Hot Work Tool Steel

NBUCOR52 / 98131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.