MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Aktiplast® ST Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Dispersant and lubricant for highly filled synthetic diene rubber compounds; particularly suitable for compounds containing high-activity silica

Use: Aktiplast ST is a processing promoter especially designed for silica compounds. It also shows excellent behavior in carbon black compounds. Aktiplast ST improves filler dispersion and reduces mixing and processing viscosities. Aktiplast ST improves scorch safety and reduces energy consumption during extrusion. Aktiplast ST improves wet grip properties (tan-d at 0 °C).

Application: Dispersant and lubricant for highly filled synthetic diene rubber compounds; particularly suitable for compounds containing high-activity silica, e.g. tire treads, technical molded articles.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
Ash 15.5 - 18.5 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 85.0 - 100 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.5 Month
 
Descriptive Properties
Appearancelight brown Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded
Envalior Stanyl® TE250F6 PA46-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America)
Röchling SUSTAMID® 46 PA 46
Overview of materials for Polyetheretherketone, Glass Fiber Filled

PLANY8254 / 208647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.