MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Mitsubishi Chemical Advanced Materials Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes:

  • Excellent chemical resistance
  • Very low moisture absorption
  • Inherently good wear and abrasion resistance
  • Unaffected by continuous exposure to hot water or steam

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.42 g/cc1.42 g/ccASTM D792
Water Absorption 0.15 %0.15 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 0.50 %0.50 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 108108ASTM D785
Hardness, Rockwell R 125125ASTM D785
Hardness, Shore D 9191ASTM D2240
Tensile Strength 110 MPa16000 psiASTM D638
Tensile Strength at 150°C (300°F) 20.7 MPa3000 psiASTM D638
Tensile Strength at 65°C (150°F) 82.7 MPa12000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 9.65 GPa1400 ksiASTM D638
Flexural Strength 159 MPa23000 psiASTM D790
Flexural Modulus 6.89 GPa1000 ksiASTM D790
Compressive Strength 193 MPa28000 psi10% Def.; ASTM D695
Compressive Modulus 4.00 GPa580 ksiASTM D695
Shear Strength 75.8 MPa11000 psiASTM D732
Izod Impact, Notched 0.747 J/cm1.40 ft-lb/inASTM D256 Type A
Coefficient of Friction, Dynamic 0.240.24Dry vs. Steel; QTM55007
K (wear) Factor 205 x 10-8 mm³/N-M102 x 10-10 in³-min/ft-lb-hrQTM 55010
Limiting Pressure Velocity 0.596 MPa-m/sec17000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1e+05<= 1e+05EOS/ESD S11.11
 
Thermal PropertiesMetricEnglishComments
CTE, linear 41.4 µm/m-°C
@Temperature -40.0 - 149 °C
23.0 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.918 W/m-K6.37 BTU-in/hr-ft²-°FASTM F433
Melting Point 340 °C644 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 249 °C480 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ColorNatural
Machinability71-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® CM GF30 Compression Molded, 30% Glass Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials Ketron® CM 1030HT PEK Polyetherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet)
Overview of materials for Polyetheretherketone, Unreinforced

P1SM17B / 20097

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.