MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain Chemfab® 1589 PTFE Coated Fiberglass Conveyor Belting
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: General Notes on Saint Gobain Open Mesh Belting Products:
CHEMFAB 1580, 1589 and 1590 are woven fiberglass belting materials designed for use in forced hot air curing ovens. Saint-Gobain Performance Plastics offers UVR versions of these products, which are designed for use in UV (ultraviolet light) curing ovens.
Dimensional Stability: Width rigidity as well as length stability is maintained by CHEMFAB Open Mesh Belting in continuous use at temperatures up to 600°F. Under normal operating tensions (3 to 10 pounds per inch of width), CHEMFAB Open Mesh Belting holds its elongation and shrinkage to less than 1%.
Release Properties: The release properties of CHEMFAB Open Mesh Belting equal or exceed those of any other available belting material. The PTFE coating makes CHEMFAB Open Mesh Belting unique in its low coefficient of friction.
Chemically Resistant:The PTFE coating encapsulates the Nomex belting carcass and enhances its useful service life.
Dynamic Strength: CHEMFAB Open Mesh Belting's durability, coupled with low overall belt weight, allows optimal production speed with decreased power requirements.
Temperature Resistant: CHEMFAB Open Mesh Belting can be operated continuously at temperatures up to 600°F and will still maintain 100% of its operational profile.
Fabrication Technology: Saint-Gobain Performance Plastics seams have been specifically engineered to reduce the flex fatigue failure. Substantially reduced flex fatigue means longer belt life. Saint-Gobain Performance Plastics offers a wide variety of seams specifically designed to reduce flex fatigue, including spiral, pin, metal and a truly endless belt. Special end reinforcements with the same properties as the belt provides durable non-fraying edge to facilitate tracking.

Notes on 1589 PTFE Coated Fiberglass Conveyor Belting:
Chemfab® 1589 is a belting material that utilizes an open mesh plain weave. This product is designed to convey small light-weight products through forced hot air ovens. Saint-Gobain Performance Plastics also manufactures a version of this product designed to be used in UV (ultra-violet light) curing ovens (called Chemfab® 1589 UVR). The substrate is fiberglass and the coating material is PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.03 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.5785 - 0.6230 g/cc0.02090 - 0.02251 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Elongation at Yield <= 1.0 %<= 1.0 %Value given for Elongation at a loading of 40 lbs/in
Tear Strength 43.8 kN/m250 pliTensile Strength (Fill)
 52.6 kN/m300 pliTensile Strength (Warp)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 316 °C600 °F
 
Descriptive Properties
Weight (oz/yd^2)13.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® 1584G PTFE Coated Fiberglass Conveyor Belting
Saint-Gobain Chemfab® 1565V PTFE Coated Fiberglass Conveyor Belting
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting

CSTGQZ104 / 2233

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.