MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Hytrel® DYM350BK TPC-ET+PBT
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door Applications

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Melt Density 1.00 g/cc
@Temperature 245 °C
0.0361 lb/in³
@Temperature 473 °F
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
 0.60 %
@Thickness 2.00 mm
0.60 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.015 cm/cm0.015 in/inISO 294-4, 2577
Melt Flow  14 g/10 min
@Load 2.16 kg,
Temperature 240 °C
14 g/10 min
@Load 4.76 lb,
Temperature 464 °F
cm³/10min Volumetric; ISO 1133
 15 g/10 min
@Load 2.16 kg,
Temperature 240 °C
15 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 3200 N
@Temperature 23.0 °C
719 lb (f)
@Temperature 73.4 °F
maximum force; ISO 6603-2
Hardness, Shore D 505015s; ISO 48-4
 <= 55<= 55ISO 48-4
Tensile Stress at Strain  10.5 MPa
@Strain 5.0 %
1520 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 13.0 MPa
@Strain 10 %
1890 psi
@Strain 10 %
ISO 527-1/-2
 16.0 MPa
@Strain 50 %
2320 psi
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 0.430 GPa62.4 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Puncture Energy 39.0 J
@Temperature 23.0 °C
28.8 ft-lb
@Temperature 73.4 °F
ISO 6603-2
Tear Strength 105 kN/m599 plinormal; ISO 34-1
 130 kN/m742 pliparallel; ISO 34-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 5.00e+14 ohm5.00e+14 ohmIEC 62631-3-2
Dielectric Constant  4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.6
@Frequency 100 Hz
4.6
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 20.0 kV/mm508 kV/inIEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 62631-2-1
 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°C100 µin/in-°FISO 11359-1/-2
Melting Point 222 °C432 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C104 °FISO 75-1/-2
Brittleness Temperature -100 °C-148 °FISO 974
Glass Transition Temp, Tg -55.0 °C-67.0 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
IEC 60695-11-10
Flame Spread 23.0 mm/min
@Thickness 1.00 mm
0.906 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 22 %22 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 245 °C473 °FOptimum, Injection
 240 - 250 °C464 - 482 °FRange, Injection
Mold Temperature 45.0 °C113 °FOptimum, Injection
 40.0 - 55.0 °C104 - 131 °FInjection
Drying Temperature 100 °C212 °FInjection
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.050 %<= 0.050 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
Emission of organic compounds (µgC/g)2.7VDA 277
FMVSS ClassSE/BISO 3795 (FMVSS 302)
Odor Class5VDA 270
Polymer(TPC+PBT)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® DYM250S BK472 TPC-ET+PBT
Celanese Hytrel® 5526 TPC-ET
Celanese Hytrel® HTR8068 TPC-ET-FR(17)
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR8341C BK320 TPC-ET

PDSX5195 / 197835

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.