MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greater
  • High Copper Peel Strength allows for thinner etched line widths
  • Lowest insertion loss available
  • Larger Panel sizes available
  • Low moisture absorption
  • Excellent CTE values lead to high reliability ceramic component attachment and PTH reliability

Benefits:

  • Mechanically strong
  • Greater dimensional stability than other 10 Dk products
  • Circuit miniaturizations leads to weight savings
  • Heat Dissipation and Management
  • Greater signal integrity
  • Cost-effective board layout and board processing
  • Low loss in humid environments

Typical Applications:

  • Ideal for X-band and below
  • Radar modules and manifolds
  • Aircraft Collision Avoidance Systems (TCAS)
  • Ground Based Radar Surveillance Systems
  • Miniaturized Circuitry & Patch Antennas
  • Power Amplifiers (PAs)
  • Low Noise Amplifiers (LNAs)

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.20 g/ccASTM D792 Method A
Water Absorption 0.030 %IPC TM-650 2.6.2.1
Outgassing - Total Mass Loss 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
Water Vapor Recovered; NASA SP-R-0022A
 0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
Collected Volatile Condensable Material 0.00 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 4300 psiCross; IPC TM-650 2.4.18.3
 5100 psiMachine; IPC TM-650 2.4.18.3
Modulus of Elasticity 200 ksiIPC TM-650 2.4.18.3
Flexural Strength 7.50 ksiCross; IPC TM-650 2.4.4
 9.90 ksiMachine; IPC TM-650 2.4.4
Compressive Modulus >= 425 ksiASTM D3410
Poissons Ratio 0.16ASTM D3039
Peel Strength >= 12.0 pliTo Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
 13.6 pliTo Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.36e+13 ohm-cmE24/125; IPC TM-650 2.5.17.1
 1.40e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 3.16e+14 ohmE24/125; IPC TM-650 2.5.17.1
 1.80e+15 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 10.2
@Frequency 1e+10 Hz
may vary by thickness; IPC TM-650 2.5.5.5
Dielectric Strength 622 V/milIPC TM-650 2.5.6.2
Dielectric Breakdown >= 45000 VIPC TM-650 2.5.6
Dissipation Factor 0.0023
@Frequency 1e+10 Hz
may vary by thickness; IPC TM-650 2.5.5.5
Arc Resistance >= 180 secIPC TM-650 2.5.1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 - 10.0 µm/m-°C
@Temperature 50.0 - 150 °C
IPC TM-650 2.4.41
CTE, linear, Transverse to Flow 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.810 W/m-KASTM E1461
Decomposition Temperature >= 500 °C5 percent; IPC TM-650 2.4.24.6
 >= 500 °COnset; IPC TM-650 2.4.24.6
Flammability, UL94 V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 60IPC TM-650 2.4.24.1
Temperature Coefficient of Dielectric (ppm/°C)-380IPC TM-650 2.5.5.5; at 10 GHz (-40 - 150°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon CLTE Microwave Printed Circuit Board Substrate
Arlon Electronic Materials 37N Polyimide Low-Flow
Arlon Electronic Materials EP2 Enhanced Polyimide Laminate and Prepreg
Arlon Electronic Materials 85N Polyimide Laminate and Prepreg
Arlon Electronic Materials 35N Fast Cure Polyimide Laminate and Prepreg

PARLM9870 / 149023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.