CLTE is a ceramic powder-filled and woven micro fiberglass reinforced PTFE composite engineered to produce a stable, low water absorption laminate with a nominal Dielectric Constant of 2.98.- Ceramic/PTFE composite
- Low water absorption
- High thermal conductivity
- Low loss
- Tight Dk and Thickness tolerance
Benefits: - Thermally stable Dk and Df
- Dimensional stability
Typical Applications: - Radar Manifolds
- Phased Array Antennas
- Microwave Feed Networks
- Phase Sensitive Electric Structures
- PAs, LNAs, LNBs
- Satellite & Space Electronics
Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |