MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ V 1082 HiPro ST ~ PEX Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ V 1082 is a translucent, high strength, two component, tin catalyzed, room temperature cure silicone rubber. It is a medium viscosity material providing excellent cured rubber properties, long library life and life-like texture. BLUESIL™ 1082 is the most flexible and softest rubber in the Bluestar Silicones mold making product line- two clear catalysts are available. HiProClear and HiPro ST~PEX, depending on eh desired hardness. BLUESIL™ V 1082 can be easily pigment4ed, which makes it ideal for robotic or animatronic skins, prosthetics, and props for theme parks and the film industry.

Applications:

  • Skins for robotic and animatronic figures for both indoor and outdoor applications
  • Special effect skins and props for the film industry
  • Theme park props and reproduction molds

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 30000 cPMixed
 40000 cPPart A, Base Component
Linear Mold Shrinkage <= 0.0020 cm/cm
@Time 86400 sec
 <= 0.0040 cm/cm
@Time 605000 sec
Storage Temperature 24.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 10ASTM D2240
Tensile Strength 550 psiASTM D412
Elongation at Break 550 %ASTM D412
Tear Strength 100 pliASTM D624, Die B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
50% RH
Pot Life 300 min
Working Life 2.00 hour
Shelf Life 36.0 Month
 
Descriptive Properties
ColorTranslucentPart A, Base Component
 TranslucentPart B, Catalyst Component
Mix Ratio10:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ CATA 3020 HT Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ CATA 3038 Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ V-1068 Silicone Rubber
Elkem (Bluestar Silicones) CAF® 530 Silicone Rubber
Borealis ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))

PBLUST050 / 191026

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.