MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elkem (Bluestar Silicones) BLUESIL™ V-1068 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL ™ V-1068 is a translucent, high strength, two component, tin catalyzed, room temperature cure silicone rubber. It is designed as a 14 Durometer (Shore A), very pourable low viscosity rubber providing excellent physical properties, long library life, and accurate detail reproduction. BLUESIL ™ V-1068 may be easily pigmented which makes it ideal for robotic and animatronic skins, special effect skins, prosthetics and props for theme parks and the film industry.

Applications:

  • Skins for robotic and animatronic figures
  • Special effect skins and props for the film industry
  • Theme park props and reproduction molds

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Viscosity 90 cP90 cPPart B, Catalyst Component
 5000 cP5000 cPPart A, Base Component
 35000 cP35000 cPMixed
Storage Temperature 24.0 °C75.2 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 121224 hr thick section
 1313ASTM D2240
Tensile Strength 3.93 MPa570 psiASTM D412
Elongation at Break 560 %560 %ASTM D412
Tear Strength 21.0 kN/m120 pliASTM D624, Die B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
50% RH
Pot Life 270 min270 min
Working Life 960 min960 min
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
ColorClearPart B, Catalyst Component
 TranslucentPart A, Base Component
Mix Ratio10:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ V 1082 HiPro ST ~ PEX Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ CATA 3020 HT Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ CATA 3038 Silicone Rubber
Overview of materials for Silicone Rubber
Dow 3120 RTV SILICONE RUBBER

PBLUST051 / 191027

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.