MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pyrotek AF-42 Spacer Bar Cover
Categories: Ceramic

Material Notes: Long service life and excellent fit have made Pyrotek's Spacer Bar Covers a highly demanded product by leaders in the extrusion heat-treating industry. Manufactured from AF-42, a synthetic textile, the covers are custom-sewn sleeves which slide over spacer bars. During heat treating and handling, these covers prevent marring by serving as an abrasion-resistant barrier between the spacer bar and stacked extrusions.

Advantages

  • Eliminates the labor costs of stacking cardboard around spacer bar. Pyrotek's Spacer Bar Covers fit over the bar's entire surface which allow the bars to be handled with greater speed.
  • Eliminates buffing costs associated with marred extrusions and scrap costs related to other cosmetic defects.
  • Long-lasting AF-42 is and economical alternative to cardboard strips.
  • Eliminates the need for clean-up of spent card-board covers.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 218 °C424 °FContinuous
Shrinkage 2.0 %
@Temperature <=218 °C
2.0 %
@Temperature <=424 °F
(Permanent) when operated at temperatures up to 218°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek B-3A REFRACTORY BOARD
Pyrotek ISOCAST Insulating Refractory Castable
Pyrotek EZ-400 Refractory Coating
Pyrotek Bonded Particle Filtration Media
Pyrotek ISOFLOW Graphite Rings Graphite Rings for Billet Casting Molds

CPYRO069 / 1808

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.