RCF. Kaowool Pumpables are water-based, pliable, puttylike materials composed of high temperature ceramic fibers, organic polymers, inorganic binders, and other proprietary ingredients. They are supplied premixed and ready to install from straight-sided 5- gallon pails using the HS-100 Extrusion or similar pump. Kaowool Pumpables can be used in hot or cold repairs of any deteriorated back-up insulation in ovens, furnaces, boilers, and process equipment, and as a hot-face repair of any cracks or gaps in existing refractory due to shrinkage. Kaowool Pumpables when dried form a hard rigid mass that provides good insulating properties, good strength and vibration resistance. Kaowool Pumpable HS – An exceptionally strong and abrasion resistant refractory insulation for applications up to 2800°F (1538°C) Applications: - Hot or cold repair to refractory backup insulation
- Hot or cold repair of boiler insulation, sidewalls,and penthouses
- Brick kiln crown and walls
- Coke oven jambs and seals
Information provided by Morgan Advanced Materials |