MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kaowool® Pumpable HS Pumpable
Categories: Ceramic; Oxide; Other Engineering Material

Material Notes: RCF. Kaowool Pumpables are water-based, pliable, puttylike materials composed of high temperature ceramic fibers, organic polymers, inorganic binders, and other proprietary ingredients. They are supplied premixed and ready to install from straight-sided 5- gallon pails using the HS-100 Extrusion or similar pump. Kaowool Pumpables can be used in hot or cold repairs of any deteriorated back-up insulation in ovens, furnaces, boilers, and process equipment, and as a hot-face repair of any cracks or gaps in existing refractory due to shrinkage. Kaowool Pumpables when dried form a hard rigid mass that provides good insulating properties, good strength and vibration resistance. Kaowool Pumpable HS – An exceptionally strong and abrasion resistant refractory insulation for applications up to 2800°F (1538°C)

Applications:

  • Hot or cold repair to refractory backup insulation
  • Hot or cold repair of boiler insulation, sidewalls,and penthouses
  • Brick kiln crown and walls
  • Coke oven jambs and seals

Information provided by Morgan Advanced Materials

Key Words: Pumpable
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.602 g/ccwet
 1.121 g/cc
@Temperature 110 °C
dried
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000614 GPa
@Temperature 110 °C
 0.00207 GPa
@Temperature 1232 °C
 0.00283 GPa
@Temperature 1399 °C
 0.00365 GPa
@Temperature 1093 °C
Compressive Strength 1.86 MPa
@Temperature 1232 °C
5% deformation, dried
 1.86 MPa
@Temperature 1399 °C
5% deformation, dried
 1.93 MPa
@Temperature 1093 °C
5% deformation, dried
 2.96 MPa
@Temperature 110 °C
5% deformation, dried
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1538 °CContinuous Use
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 - 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Al2O3 47 - 50 %
Fe2O3 0.40 - 0.70 %
Other 2.0 - 4.0 %
SiO2 47 - 50 %
 
Descriptive Properties
Classification Temperature (°C)1538
Colorlight brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Ropes Twisted Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber

CMORF6158 / 202942

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.