MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemours Teflon® PFA Grade 335 Aqueous Dispersion  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon® PFA 335 (formerly TE-9946) is a negatively charged, hydrophobic colloid, containing approximately 60% (by total weight) of 0.05 to 0.5 µm perfluoroalkoxy (PFA) resin particles suspended in water. A milky white liquid, Teflon® PFA 335 also contains approximately 5% by weight of a nonionic wetting agent and stabilizer (based on the weight of the PFA solids). Viscosity at room temperature is approximately 20 cP. Nominal pH is 10.

Unlike Teflon® PTFE dispersions, the resin in Teflon® PFA 335 is a true thermoplastic and will exhibit some flow above its melting point. When properly processed, the PFA resin in Teflon® PFA 335 exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Teflon® PFA 335 is a general-purpose product used in a variety of coating applications. It can also be used as a heat sealable topcoat.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D4441
Base Resin Density 0.900 g/cc0.0325 lb/in³Weight of PFA Resin Solids; ASTM D4441
Solids Content 60 %60 %Percent PFA Resin Solids; ASTM D4441
Particle Size 0.20 µm0.20 µm
pH 9.59.5ASTM E70
Viscosity 20 cP
@Temperature 25.0 °C
20 cP
@Temperature 77.0 °F
ASTM D2196
Melt Flow 1.0 - 3.0 g/10 min1.0 - 3.0 g/10 minASTM D3307
 
Thermal PropertiesMetricEnglishComments
Melting Point 305 °C581 °FPeak Temperature; ASTM D1457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Chemours Teflon® PFA Grade 440 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 450 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin
Chemours 340 PFA Perfluoroalkoxy Copolymer

PDU9229 / 33342

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.