MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Teflon® PFA 345 is a medium-flow-rate resin available in clear 2.5-mm (0.1-in.) pellets. Compared with Teflon® PFA 340, it offers increased flex life and greater resistance to environmental stress cracking.

All grades of Teflon® PFA combine the processing ease of conventional thermoplastics with properties similar to those of Teflon® PTFE fluorocarbon resin. They have high melt strength, stability at high processing temperatures, and resistance to creep at high service temperatures.

Teflon® PFA retains its properties after service at 260°C (500°F) and has useful properties at temperatures as low as –196°C (–320°F). It is inert to nearly all industrial chemicals and solvents, and its dielectric properties are excellent. Products madewith Teflon® PFA have moderate stiffness and high elongation.

In a flame situation, products of Teflon® PFA resist ignition and do not themselves promote flame spread. When ignited by flame from other sources, their contribution of heat is very small and added at a slow rate with very little smoke.

Applications

Applications for Teflon® PFA 345 include tubing; wire and cable insulation; injection-molded parts; and chemically resistant linings for bellows, valves, fittings, pipes, pumps, and other fluid- handling components.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %24 hours; ASTM D570
Melt Flow 4.1 - 8.9 g/10 min4.1 - 8.9 g/10 minASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength, Ultimate 29.0 MPa4210 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Flexural Modulus 0.690 GPa100 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.1
@Frequency 60.0 - 1.00e+9 Hz
2.1
@Frequency 60.0 - 1.00e+9 Hz
ASTM D150
Dielectric Strength >= 80.0 kV/mm
@Thickness 0.0250 mm
>= 2030 kV/in
@Thickness 0.000984 in
film; ASTM D149
Dissipation Factor 0.00020 - 0.0010
@Frequency 60.0 - 1.00e+9 Hz
0.00020 - 0.0010
@Frequency 60.0 - 1.00e+9 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 200 µm/m-°C
@Temperature 100 - 149 °C
66.7 - 111 µin/in-°F
@Temperature 212 - 300 °F
ASTM D696
Melting Point 305 °C581 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °F
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 379 - 399 °C714 - 750 °FCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm100000
Heat of Combustion J/g5300ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance10Years unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Teflon® PFA Grade 450 HP Extrusion and Molding Resin
Chemours Teflon® FEP 5100 Fluoropolymer Resin
Chemours Teflon® PFA Grade 440 HP Extrusion and Molding Resin
Chemours Teflon® PFA Grade 345T Extrusion and Molding Resin for High Temperature Applications
Chemours Teflon® PFA Grade 940 HP Plus Extrusion and Molding Resin

PDU921A / 33332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.