MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: MULTICLAD™ HF represents the next generation low-loss thermoset and prepreg system for high-speed and high-frequency printed circuit boards. This technology combines a low-loss, high reliability thermoset resin system with non-brominated flame retardant system to create a material that is great in terms of electrical performance, durability and cost.

  • First generation environmentally friendly laminate system with competitive Insertion Loss and Loss Tangent (Df < 0.005) for High Frequency applications
  • Non-PTFE Formulation meets standard lead-free process requirements, while maintaining low-halogen content per current industry standards
  • Improved thermal robustness cover competing low-loss thermoset materials for better device reliability and performance consistency over time
  • Low Thermal Expansion and High Glass Transition Temperature minimizes potential for PTH failures and improves operating reliability
  • Low moisture absorption for improved processing and consistent performance
  • Decomposition temperature > 350°C is ideally suited for lead-free solder processing
  • Low TCEr (temperature coefficient of the dielectric) minimizes electrical phase variation with temperature
  • Certified to UL flammability requirements of UL-94 V0

Typical Applications:

  • High-Speed Digital backplanes and server boards
  • RF Power Amplifier motherboards
  • Satellite receivers, LNB converters, and other Wireless devices
  • Semiconductor burn-in-boards and other high speed, high reliability applications

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ASTM D792 Method A
Water Absorption 0.10 %0.10 %IPC TM-650 2.6.2.1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.9 MPa10000 psiCross; IPC TM-650 2.4.18.3
 101 MPa14700 psiMachine; IPC TM-650 2.4.18.3
Modulus of Elasticity 20.7 GPa3000 ksiIPC TM-650 2.4.4
Flexural Strength 223 MPa32300 psiCross; IPC TM-650 2.4.18.3
 273 MPa39600 psiMachine; IPC TM-650 2.4.18.3
Compressive Modulus 2.92 GPa424 ksiASTM D3410
Poissons Ratio 0.280.28x,y; ASTM D3039
Peel Strength 1.40 kN/m8.00 pliTo Copper (1 oz/35 micron); After Process Solutions; IPC TM-650 2.4.8
 1.49 kN/m8.50 pliTo Copper (1 oz/35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
 1.58 kN/m9.00 pliTo Copper (1 oz/35 micron); After Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.40e+14 ohm-cm1.40e+14 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
 5.00e+14 ohm-cm5.00e+14 ohm-cmE24/125; IPC TM-650 2.5.17.1
Surface Resistance 3.00e+13 ohm3.00e+13 ohmC96/35/90; IPC TM-650 2.5.17.1
 6.00e+13 ohm6.00e+13 ohmE24/125; IPC TM-650 2.5.17.1
Dielectric Constant  3.7
@Frequency 1e+9 Hz
3.7
@Frequency 1e+9 Hz
IPC TM-650 2.5.5.5
 3.75
@Frequency 1e+6 Hz
3.75
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
Dielectric Strength 39.4 kV/mm1000 kV/inIPC TM-650 2.5.6.2
Dielectric Breakdown 36500 V36500 VIPC TM-650 2.5.6
Dissipation Factor  0.0040
@Frequency 1e+6 Hz
0.0040
@Frequency 1e+6 Hz
IPC TM-650 2.5.5.3
 0.0045
@Frequency 1e+9 Hz
0.0045
@Frequency 1e+9 Hz
IPC TM-650 2.5.5.5
Arc Resistance 190 sec190 secIPC TM-650 2.5.1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 - 16.0 µm/m-°C7.78 - 8.89 µin/in-°Fx,y direction; IPC TM-650 2.4.41
CTE, linear, Transverse to Flow  20.0 µm/m-°C
@Temperature <=190 °C
11.1 µin/in-°F
@Temperature <=374 °F
z (< Tg); IPC TM-650 2.4.24
 150 µm/m-°C
@Temperature >=190 °C
83.3 µin/in-°F
@Temperature >=374 °F
z (> Tg); IPC TM-650 2.4.24
Thermal Conductivity 0.640 W/m-K4.44 BTU-in/hr-ft²-°FASTM E1461
Glass Transition Temp, Tg 190 °C374 °FTMA; IPC TM-650 2.4.24
 205 °C401 °FDSC; IPC TM-650 2.4.25
Decomposition Temperature 390 °C734 °FInitial; IPC TM-650 2.3.41
 432 °C810 °F5 percent; IPC TM-650 2.3.41
Flammability, UL94 V-0V-0
 
Descriptive Properties
IPC Delamination - T260 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T288 (minutes)> 60IPC TM-650 2.4.24.1
IPC Delamination - T300 (minutes)> 60IPC TM-650 2.4.24.1
Temperature Coefficient of Dielectric (ppm/°C)75IPC TM-650 2.5.5.5; at 10 GHz, 0-140°C
Z-Axis Expansion (%)1.2IPC TM-650 2.4.24 (50-260°C)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® H 4320 Q600 POM
Overview of materials for Polyetherimide (PEI)
Rogers Arlon AD300C Commercial Microwave and RF Laminate Material
BASF Ultradur® B 6550 PBT
BASF Ultradur® B 6550 LN PBT

PARLM9857 / 149010

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.