MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NeoGraf GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced
Categories: Carbon; Graphite

Material Notes: GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. The polymer facing enhances product handleability and durability, making GRAFKOTE® laminates an excellent gasketing material. Each laminate is surface identifiable, branded with the GRAFOIL® grade. Its applications include: valves, pumps, pipe/ASME/API/DIN flanges, glass-lined or low load flange equipment, steam traps, heat exchangers, and compressors. The advantages of GRAFKOTE® products are: compatible with many chemicals; maximum continuous use temperature 400°C (750°F); no shelf life; material availability in rolls allows for maximum material utilization; easily cut; contains no hazardous materials; improved handleability and durability; superior to non-asbestos fiber sheet in every characteristic (Creep, Recovery, and Sealability). Single-Sided Laminate Construction: 0.0005" thick polymer ? GRAFOIL® Grade GTB. Double-Sided Laminate Construction: 0.0005" thick polymer ? GRAFOIL® Grade GTB ? 0.0005" thick polymer.

Formerly a product of GrafTech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 70.0 lb/ft³Standard; Graphite
Thickness 760 micronsStandard for Single-Sided Laminate
 1520 micronsStandard for Single-Sided Laminate
 1570 micronsStandard for Double-Sided Laminate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 800 psi>= 0.030" Thick
 950 psi0.010" Thick
Compression Set 80 %
@Pressure 34.5 MPa
after 5000 psi load
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C0.010", 0.017" thick
 400 °C0.030", 0.060", 0.062", 0.082" thick
 
Descriptive Properties
"m" Factor2ASME Gasket Factor
"y" Stress (psi)900ASME Gasket Factor
Compressibility (%)43at 5000 psi load
Max Gasket Unit Load (psi)6526ASME Gasket Factor

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NeoGraf GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
NeoGraf GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material
NeoGraf GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced
NeoGraf GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material

CGRAF934 / 107338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.