MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

JIS SKH3 Tungsten High Speed Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Used in high speed tool and cutting applications such as drills, milling processes, reamers, etc. Tungsten content promotes high temperature hardness and wear resistance.

Key Words: JIS G4403(83) SKH3, SKH 3, SKH-3. Comparable to AISI T4 Tool Steel, UNS T12004
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.68 g/cc0.314 lb/in³(AISI T4)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 269<= 269Bar Forging Annealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.9 µm/m-°C
@Temperature 20.0 - 540 °C
6.61 µin/in-°F
@Temperature 68.0 - 1000 °F
(AISI T4)
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.73 - 0.83 %0.73 - 0.83 %
Chromium, Cr 3.8 - 4.5 %3.8 - 4.5 %
Cobalt, Co 4.5 - 5.5 %4.5 - 5.5 %
Copper, Cu <= 0.25 %<= 0.25 %
Iron, Fe 66.8 - 72.8 %66.8 - 72.8 %As Balance
Manganese, Mn <= 0.40 %<= 0.40 %
Nickel, Ni <= 0.25 %<= 0.25 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 0.40 %<= 0.40 %
Sulfur, S <= 0.030 %<= 0.030 %
Tungsten, W 17 - 19 %17 - 19 %
Vanadium, V 0.80 - 1.2 %0.80 - 1.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
JIS SK1 Water Hardening Tool Steel
JIS SHK55 Molybdenum High Speed Tool Steel
JIS SCM435 Chromium Molybdenum Steel
JIS S55C Steel, Tempered
JIS S55C Steel, Normalized

MSTZJSKH3 / 231114

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.