MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Overview of materials for Polycarbonate, Gamma Radiation Resistant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Gamma Radiation Resistant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.19 - 1.21 g/ccAverage value: 1.20 g/cc Grade Count:50
Water Absorption 0.140 - 0.350 %Average value: 0.194 % Grade Count:34
Moisture Absorption at Equilibrium 0.0200 - 0.350 %Average value: 0.195 % Grade Count:33
 0.580 - 0.580 %
@Temperature 100 - 100 °C
Average value: 0.580 % Grade Count:5
Water Absorption at Saturation 0.160 - 0.350 %Average value: 0.202 % Grade Count:12
Viscosity 3.00 - 33.0 cP
@Temperature 300 - 330 °C
Average value: 14.3 cP Grade Count:11
 3.00 - 33.0 cP
@Load 1.20 - 2.16 kg
Average value: 14.3 cP Grade Count:11
Linear Mold Shrinkage 0.00400 - 0.00800 cm/cmAverage value: 0.00623 cm/cm Grade Count:48
Linear Mold Shrinkage, Transverse 0.00400 - 0.00800 cm/cmAverage value: 0.00600 cm/cm Grade Count:13
Melt Flow 3.00 - 35.0 g/10 minAverage value: 14.9 g/10 min Grade Count:49
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70.0 - 85.0Average value: 76.0 Grade Count:23
Hardness, Rockwell R 118 - 122Average value: 119 Grade Count:30
Ball Indentation Hardness 95.0 MPaAverage value: 95.0 MPa Grade Count:6
Tensile Strength, Ultimate 46.9 - 74.0 MPaAverage value: 66.2 MPa Grade Count:45
Tensile Strength, Yield 59.0 - 65.5 MPaAverage value: 62.9 MPa Grade Count:50
Elongation at Break 50.0 - 180 %Average value: 114 % Grade Count:50
Elongation at Yield 5.40 - 7.00 %Average value: 6.39 % Grade Count:46
Modulus of Elasticity 2.09 - 2.50 GPaAverage value: 2.29 GPa Grade Count:38
Flexural Yield Strength 66.0 - 100 MPaAverage value: 91.0 MPa Grade Count:46
Flexural Modulus 2.02 - 2.41 GPaAverage value: 2.25 GPa Grade Count:44
Izod Impact 600 - 702 JAverage value: 640 J Grade Count:11
 120 - 220 J
@Temperature -30.0 - -30.0 °C
Average value: 151 J Grade Count:11
Izod Impact, Notched 0.981 - 750 J/cmAverage value: 28.6 J/cm Grade Count:28
 2.20 - 7.85 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 5.03 J/cm Grade Count:6
Izod Impact, Unnotched 27.0 J/cm - NBAverage value: 31.0 J/cm Grade Count:19
Izod Impact, Notched (ISO) 12.0 - 78.0 kJ/m²Average value: 47.5 kJ/m² Grade Count:32
 10.0 - 15.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 11.1 kJ/m² Grade Count:23
Izod Impact, Unnotched (ISO) NBGrade Count:22
 NB - NB
@Temperature -30.0 - -30.0 °C
Grade Count:17
Charpy Impact Unnotched 1000 J/cm² - NBGrade Count:20
 999.9 - 999.9 J/cm²
@Temperature -30.0 - -30.0 °C
Grade Count:14
Charpy Impact, Notched 1.00 - 8.20 J/cm²Average value: 4.72 J/cm² Grade Count:35
 1.00 - 1.50 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 1.34 J/cm² Grade Count:17
Gardner Impact 36.2 JAverage value: 36.2 J Grade Count:8
Tensile Impact Strength 378 - 577 kJ/m²Average value: 481 kJ/m² Grade Count:21
Dart Drop, Total Energy 54.0 - 149 JAverage value: 97.4 J Grade Count:27
Falling Dart Impact 169 JAverage value: 169 J Grade Count:5
Taber Abrasion, mg/1000 Cycles 10.0 - 32.0Average value: 12.8 Grade Count:8
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 - 2.60e+17 ohm-cmAverage value: 1.20e+17 ohm-cm Grade Count:28
Surface Resistance 1.00e+15 - 6.00e+15 ohmAverage value: 2.43e+15 ohm Grade Count:14
Dielectric Constant 2.70 - 3.17Average value: 2.95 Grade Count:22
Dielectric Strength 14.9 - 35.0 kV/mmAverage value: 18.4 kV/mm Grade Count:22
Dissipation Factor 0.000100 - 0.0240Average value: 0.00709 Grade Count:22
Comparative Tracking Index 125 - 250 VAverage value: 203 V Grade Count:4
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/minAverage value: 115 mm/min Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 59.4 - 91.8 µm/m-°CAverage value: 69.1 µm/m-°C Grade Count:37
CTE, linear, Transverse to Flow 60.0 - 80.0 µm/m-°CAverage value: 68.6 µm/m-°C Grade Count:22
Specific Heat Capacity 1.25 - 1.26 J/g-°CAverage value: 1.25 J/g-°C Grade Count:14
Thermal Conductivity 0.190 - 0.210 W/m-KAverage value: 0.202 W/m-K Grade Count:17
Maximum Service Temperature, Air 120 °CAverage value: 120 °C Grade Count:4
Hot Ball Pressure Test 75.0 - 140 °CAverage value: 117 °C Grade Count:16
Deflection Temperature at 0.46 MPa (66 psi) 124 - 145 °CAverage value: 136 °C Grade Count:32
Deflection Temperature at 1.8 MPa (264 psi) 117 - 143 °CAverage value: 129 °C Grade Count:47
Vicat Softening Point 137 - 160 °CAverage value: 147 °C Grade Count:42
Minimum Service Temperature, Air -40.0 °CAverage value: -40.0 °C Grade Count:4
UL RTI, Electrical 80.0 - 125 °CAverage value: 114 °C Grade Count:4
UL RTI, Mechanical with Impact 80.0 - 125 °CAverage value: 114 °C Grade Count:4
UL RTI, Mechanical without Impact 80.0 - 125 °CAverage value: 114 °C Grade Count:4
Flammability, UL94 HB - V-2Grade Count:16
Oxygen Index 25.0 %Average value: 25.0 % Grade Count:8
Glow Wire Test 850 °CAverage value: 850 °C Grade Count:3
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.59 - 1.60Average value: 1.59 Grade Count:20
Haze 0.600 - 3.00 %Average value: 1.11 % Grade Count:31
Transmission, Visible 82.0 - 89.0 %Average value: 86.3 % Grade Count:24
UV Transmittance 88.0 %Average value: 88.0 % Grade Count:8
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CAverage value: 70.0 °C Grade Count:6
Nozzle Temperature 265 - 355 °CAverage value: 304 °C Grade Count:25
Melt Temperature 249 - 360 °CAverage value: 299 °C Grade Count:33
Mold Temperature 65.6 - 116 °CAverage value: 89.2 °C Grade Count:33
Drying Temperature 118 - 124 °CAverage value: 120 °C Grade Count:33
Moisture Content 0.0200 %Average value: 0.0200 % Grade Count:14
Vent Depth 0.00127 - 0.00760 cmAverage value: 0.00393 cm Grade Count:27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
Overview of materials for Polycarbonate, 10% Glass Filled
Overview of materials for Polycarbonate, PTFE Filled
Overview of materials for Polycarbonate, UV Stabilized
Overview of materials for Polycarbonate, Optical Grade

O3109 / 78128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.