MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 52G1 V20 PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled parts

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This grade is Halogen and Red Phosphorous free fire resistant flame retardant grade is particularly suitable for equipment requiring robust glow-wire resistance with excellent molding and electrical performance, such as for MCB housings, contactors and switches and sockets. This grade is available in Grey, White, Natural and Black colors. Laser marking grades and other colors are available upon request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 92.0 MPaISO 527 Type 1A
Elongation at Break 2.9 %ISO 527 Type 1A
Tensile Modulus 6700 MPaISO 527 Type 1A
Charpy Impact Unnotched 39.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 3.10 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 3.20 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 31.0 kV/mmIEC 60243
Comparative Tracking Index 450 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 170 °CISO 75/Af
Flammability, UL94 V-2
@Thickness 0.800 mm
1210
 V-2
@Thickness 1.60 mm
1210
 V-2
@Thickness 3.20 mm
1210
Oxygen Index 29 %ISO 4589
Glow Wire Ignition Temperature 700 °C
@Thickness 1.60 mm
ISO 60695-2-13
 725 °C
@Thickness 0.800 mm
ISO 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 220 - 230 °C
Front Barrel Temperature 245 - 255 °C
Mold Temperature 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® C 52G1 V20 PA6, Conditioned
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced
Domo TECHNYL® C 507XT PA6, Conditioned
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Envalior Durethan® DP BC 310 EF 000000 Nylon 6

PRHOD793 / 138024

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.