MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Domo TECHNYL® C 52G1 V20 PA6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled parts

Available in: Asia Pacific, Europe, Latin America and North America

Product Applications: This grade is Halogen and Red Phosphorous free fire resistant flame retardant grade is particularly suitable for equipment requiring robust glow-wire resistance with excellent molding and electrical performance, such as for MCB housings, contactors and switches and sockets. This grade is available in Grey, White, Natural and Black colors. Laser marking grades and other colors are available upon request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.32 g/cc0.0477 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 65.0 MPa9430 psiISO 527 Type 1A
Elongation at Break 4.8 %4.8 %ISO 527 Type 1A
Tensile Modulus 4.55 GPa660 ksiISO 527 Type 1A
Charpy Impact Unnotched 7.90 J/cm²37.6 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched  0.340 J/cm²
@Temperature -30.0 °C
1.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.860 J/cm²
@Temperature 23.0 °C
4.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced
Domo TECHNYL® C 52G1 V20 PA6, DRY
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
Techmer ES HiFill® PA6 0303 B
Plastcom PLASTAMID® 6HM PA6

PRHOD794 / 138025

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.