MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin EM6100 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ EM6100 is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This grade exhibits a balance of flow/heat/impact, dimensional stability, along with paint adhesion. NORYL EM6100 resin is suitable for the automotive interior market in applications such as HVAC housings and radio components. MS-DB424, WSBM4D844-A9, GMP.PPE.007.

Features: Good Mold Release,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Water Absorption 0.20 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Viscosity 15 cP
@Load 5.00 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaASTM D638
 40.0 MPaISO 527
Tensile Strength, Yield 42.0 MPaISO 527
 43.0 MPa50 mm/min; ASTM D638
Elongation at Break 60 %ISO 527
 65 %50 mm/min; ASTM D638
Elongation at Yield 2.8 %ISO 527
 3.0 %ASTM D638
Tensile Modulus 1900 MPa5 mm/min; ASTM D638
 2050 MPa1 mm/min; ISO 527
Flexural Strength 65.0 MPaISO 178
 66.0 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
 67.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2000 MPa2.6 mm/min, 100 mm span; ASTM D790
 2100 MPa1.3 mm/min, 50 mm span; ASTM D790
 2100 MPaISO 178
Izod Impact Notched 453 JASTM D256
 250 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 33.0 kJ/m²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 33.0 kJ/m²ISO 179/2C
 19.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 36.0 Jpeak; ASTM D3763
 42.0 JASTM D3763
 24.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 117 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 126 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 124 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 106 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 115 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 119 °CRate B/50; ISO 306
 123 °CRate B/120; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 265 - 295 °C
Zone 2 245 - 290 °C
Zone 3 255 - 295 °C
Melt Temperature 265 - 295 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Vent Depth 0.00380 - 0.00510 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82271 / 290218

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.