MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC NORYL™ Resin EM6100 Polyphenylene Ether + PS (PPE+PS) (Europe)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ EM6100 is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This grade exhibits a balance of flow/heat/impact, dimensional stability, along with paint adhesion. NORYL EM6100 resin is suitable for the automotive interior market in applications such as HVAC housings and radio components. MS-DB424, WSBM4D844-A9, GMP.PPE.007.

Features: Good Mold Release,Antistatic

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity 15 cP
@Load 5.00 kg,
Temperature 280 °C
15 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 280 °C
15 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiASTM D638
 40.0 MPa5800 psiISO 527
Tensile Strength, Yield 42.0 MPa6090 psiISO 527
 43.0 MPa6240 psi50 mm/min; ASTM D638
Elongation at Break 60 %60 %ISO 527
 65 %65 %50 mm/min; ASTM D638
Elongation at Yield 2.8 %2.8 %ISO 527
 3.0 %3.0 %ASTM D638
Tensile Modulus 1.90 GPa276 ksi5 mm/min; ASTM D638
 2.05 GPa297 ksi1 mm/min; ISO 527
Flexural Strength 65.0 MPa9430 psiISO 178
 66.0 MPa9570 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
 67.0 MPa9720 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.00 GPa290 ksi2.6 mm/min, 100 mm span; ASTM D790
 2.10 GPa305 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.10 GPa305 ksiISO 178
Izod Impact Notched 453 J334 ft-lbASTM D256
 250 J
@Temperature -30.0 °C
184 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 33.0 kJ/m²15.7 ft-lb/in²80*10*4; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 3.30 J/cm²15.7 ft-lb/in²ISO 179/2C
 1.90 J/cm²
@Temperature -30.0 °C
9.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179/2C
Dart Drop, Total Energy 36.0 J26.6 ft-lbpeak; ASTM D3763
 42.0 J31.0 ft-lbASTM D3763
 24.0 J
@Temperature -30.0 °C
17.7 ft-lb
@Temperature -22.0 °F
peak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 117 µm/m-°C
@Temperature 0.000 - 100 °C
65.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 126 °C259 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 124 °C
@Thickness 3.20 mm
255 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C230 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 106 °C
@Thickness 3.20 mm
223 °F
@Thickness 0.126 in
unannealed; ASTM D648
 115 °C
@Thickness 6.40 mm
239 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 119 °C246 °FRate B/50; ISO 306
 123 °C253 °FRate B/120; ISO 306
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 295 °C509 - 563 °F
Zone 2 245 - 290 °C473 - 554 °F
Zone 3 255 - 295 °C491 - 563 °F
Melt Temperature 265 - 295 °C509 - 563 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82271 / 290218

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.