MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R550HT BK02 Nylon 66, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Vydyne R550HT BK02 is a 50% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. It was specifically developed to withstand long term exposure to elevated temperatures up to 190°C. R550HT BK02 offers improved flow with an improved black surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccDAM; ISO 1183
Water Absorption 1.1 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.2 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 161 MPa50% RH; ISO 527-2
 230 MPaDAM; ISO 527-2
Elongation at Break 2.5 %DAM; ISO 527-2
 3.5 %50% RH; ISO 527-2
Tensile Modulus 12000 MPa50% RH; ISO 527-2
 17000 MPaDAM; ISO 527-2
Flexural Strength 215 MPa50% RH; ISO 178
 350 MPaDAM; ISO 178
Flexural Modulus 10500 MPa50% RH; ISO 178
 15700 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 16.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 16.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 16.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 97.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 100 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 110 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 120 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 22.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 253 °CUnannealed; 50% RH; ISO 75-2/B
 256 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 239 °CUnannealed; 50% RH; ISO 75-2/A
 246 °CUnannealed; DAM; ISO 75-2/A
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
ISO 3795
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D6779 PA012G50
AppearanceBlack
FeaturesGood Mold Release
 Heat Stabilized
 High Flow
 High Rigidity
 High Strength
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ascend Performance Materials Vydyne® R535HT BK653 Nylon 66, 35% Glass Filled
Ascend Performance Materials Vydyne® R535H BK02 Nylon 66, 35% Glass Filled

PASCE9845 / 220946

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.