Physical Properties | Metric | English | Comments |
---|
Density | 1.59 g/cc | 0.0574 lb/in³ |
Water Absorption | 1.1 % @Time 86400 sec | 1.1 % @Time 24.0 hour |
Moisture Absorption at Equilibrium | 1.2 % | 1.2 % |
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm | 0.0030 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.0080 cm/cm @Thickness 2.00 mm | 0.0080 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 161 MPa | 23400 psi |
| 230 MPa | 33400 psi |
Elongation at Break | 2.5 % | 2.5 % |
| 3.5 % | 3.5 % |
Tensile Modulus | 12.0 GPa | 1740 ksi |
| 17.0 GPa | 2470 ksi |
Flexural Strength | 215 MPa | 31200 psi |
| 350 MPa | 50800 psi |
Flexural Modulus | 10.5 GPa | 1520 ksi |
| 15.7 GPa | 2280 ksi |
Poissons Ratio | 0.40 | 0.40 |
Izod Impact, Notched (ISO) | 16.0 kJ/m² @Temperature -40.0 °C | 7.61 ft-lb/in² @Temperature -40.0 °F |
| 16.0 kJ/m² @Temperature -40.0 °C | 7.61 ft-lb/in² @Temperature -40.0 °F |
| 16.0 kJ/m² @Temperature -30.0 °C | 7.61 ft-lb/in² @Temperature -22.0 °F |
| 16.0 kJ/m² @Temperature -30.0 °C | 7.61 ft-lb/in² @Temperature -22.0 °F |
| 16.0 kJ/m² @Temperature 23.0 °C | 7.61 ft-lb/in² @Temperature 73.4 °F |
| 20.0 kJ/m² @Temperature 23.0 °C | 9.52 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | 9.70 J/cm² @Temperature 23.0 °C | 46.2 ft-lb/in² @Temperature 73.4 °F |
| 10.0 J/cm² @Temperature -40.0 °C | 47.6 ft-lb/in² @Temperature -40.0 °F |
| 10.0 J/cm² @Temperature -40.0 °C | 47.6 ft-lb/in² @Temperature -40.0 °F |
| 10.0 J/cm² @Temperature -30.0 °C | 47.6 ft-lb/in² @Temperature -22.0 °F |
| 11.0 J/cm² @Temperature -30.0 °C | 52.3 ft-lb/in² @Temperature -22.0 °F |
| 12.0 J/cm² @Temperature 23.0 °C | 57.1 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 1.50 J/cm² @Temperature -40.0 °C | 7.14 ft-lb/in² @Temperature -40.0 °F |
| 1.50 J/cm² @Temperature -40.0 °C | 7.14 ft-lb/in² @Temperature -40.0 °F |
| 1.50 J/cm² @Temperature -30.0 °C | 7.14 ft-lb/in² @Temperature -22.0 °F |
| 1.50 J/cm² @Temperature -30.0 °C | 7.14 ft-lb/in² @Temperature -22.0 °F |
| 1.60 J/cm² @Temperature 23.0 °C | 7.61 ft-lb/in² @Temperature 73.4 °F |
| 2.20 J/cm² @Temperature 23.0 °C | 10.5 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Strength | 29.0 kV/mm @Thickness 1.00 mm | 737 kV/in @Thickness 0.0394 in |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 253 °C | 487 °F |
| 256 °C | 493 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 239 °C | 462 °F |
| 246 °C | 475 °F |
Flame Spread | 0.000 mm/min @Thickness 2.00 mm | 0.000 in/min @Thickness 0.0787 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Middle Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Front Barrel Temperature | 280 - 310 °C | 536 - 590 °F |
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F |
Melt Temperature | 285 - 305 °C | 545 - 581 °F |
Mold Temperature | 65.0 - 95.0 °C | 149 - 203 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 hour | 4.00 hour |
|
Descriptive Properties |
---|
Additive | Heat Stabilizer |
| Lubricant |
Agency Ratings | ASTM, D6779 PA012G50 |
Appearance | Black |
Features | Good Mold Release |
| Heat Stabilized |
| High Flow |
| High Rigidity |
| High Strength |
| Lubricated |
Forms | Pellets |
Processing Method | Injection Molding |
Region | North America, Europe, Asia Pacific |
UL File Number | E70062 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.