MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Type P-VS-0053 (Union Carbide) Carbon Fiber
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite

Material Notes: Pitch fibers are prepared by heating aromatic compounds above 350°C. A dehydrogenation condensation reaction occurs to form planar aromatic molecules which aggregate into a liquid crystalline phase (a mesophase). Once the mesophase content has reached about 40%, a phase inversion occurs and this anisotropic material becomes the continuous phase.

Key Words: composites, fibers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 2000 MPa290000 psiFiber only. Composites containing this fiber may have tensile strength of 1000 MPa.
Modulus of Elasticity 300 GPa43500 ksior 520 GPa for fiber
Shear Strength 20.0 MPa2900 psiInterlaminar shear.

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Thornel® P-100 Carbon Fiber/Epoxy Advanced Composite System
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite
Henkel Hysol Benzoxazine 99110 Infusion Resin
Phenolic 40%, Carbon fabric 60%

PCO005 / 28595

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.