MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Hysol Benzoxazine 99110 Infusion Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: One-part Infusion resin for RTM & VARTM processing. Low viscosity, high hot-wet properties and very good resistance against flame, smoke and toxicity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 23.0 °C73.4 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 71.0 MPa10300 psi
Elongation at Break 1.5 %1.5 %
Tensile Modulus 3.70 GPa537 ksi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Glass Transition Temp, Tg 161 °C322 °FWet - 72 Hour Boil
 191 °C376 °FDry
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min
@Temperature 180 °C
1.50 hour
@Temperature 356 °F
Pot Life 259000 min259000 min
 
Descriptive Properties
ConsistencyLow Viscosity
Form1 part
Fracture Toughness (J/m2)112

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol Benzoxazine 99120 Infusion Resin
Solvay CYCOM® 7714A Epoxy - Unidirectional Carbon Tape and Roving Composite
Solvay CYCOM® 977-20 Resin System with PRIFORM™ Technology
Toyobo Zylon® HM Fiber/Epoxy Matrix Unidirectional Composite
Solvay CYCOM® 977-3 Neat Epoxy Resin

PHENK827 / 146832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.