MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Morgan Advanced Ceramics Kaolite Super HS Gun Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Gun installation. Kaolite Super HS Gun is a medium weight, premium insulating monolithic for use up to 2400°F (1371°C). It has exceptional strength to weight characteristics and is well suitable for tough petrochemical F.C.C.U. applications.

Applications:

  • Backup insulation in two component linings in petrochemical process units
  • Hot face lining in ductwork from waste heat recovery boilers and process unit
  • F.C.C.U. linings - regenerator
  • Hydrogen or reducing atmosphere linings
  • Radiant section in steam flood generators
  • Steam flood generator convection sections and target walls
  • Cat cracker regenerator lining

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.154 - 1.33 g/cc
@Temperature 816 °C
0.04169 - 0.0480 lb/in³
@Temperature 1500 °F
fired
 1.281 - 1.458 g/cc
@Temperature 104 °C,
Time 86400 sec
0.04628 - 0.05267 lb/in³
@Temperature 219 °F,
Time 24.0 hour
dried
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00138 - 0.00414 GPa0.200 - 0.600 ksifired 5 hours at 816°C
 0.00310 - 0.00621 GPa0.450 - 0.901 ksidried 24 hours at 104°C
 0.00344 - 0.00690 GPa0.499 - 1.00 ksifired 5 hours at temp use limit, °C
Compressive Strength  12.4 - 24.1 MPa
@Temperature 1093 °C,
Time 18000 sec
1800 - 3500 psi
@Temperature 1999 °F,
Time 5.00 hour
Cold Crushing Strength, fired
 15.1 - 34.5 MPa
@Temperature 104 °C,
Time 86400 sec
2190 - 5000 psi
@Temperature 219 °F,
Time 24.0 hour
Cold Crushing Strength, dried
 17.2 - 34.5 MPa
@Temperature 1315 °C,
Time 18000 sec
2490 - 5000 psi
@Temperature 2399 °F,
Time 5.00 hour
Cold Crushing Strength, fired
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.390 W/m-K
@Temperature 260 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
 0.420 W/m-K
@Temperature 538 °C
2.91 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 0.430 W/m-K
@Temperature 815 °C
2.98 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
 0.460 W/m-K
@Temperature 1093 °C
3.19 BTU-in/hr-ft²-°F
@Temperature 1999 °F
ASTM C201
Maximum Service Temperature, Air <= 1315 °C<= 2399 °F
Shrinkage  0.00 - 0.20 %
@Treatment Temp. 104 °C,
Time 86400 sec
0.00 - 0.20 %
@Treatment Temp. 219 °F,
Time 24.0 hour
dried; ASTM C113
 0.10 - 0.40 %
@Treatment Temp. 1093 °C,
Time 18000 sec
0.10 - 0.40 %
@Treatment Temp. 1999 °F,
Time 5.00 hour
fired; ASTM C113
 0.50 - 1.5 %
@Treatment Temp. 1315 °C,
Time 18000 sec
0.50 - 1.5 %
@Treatment Temp. 2399 °F,
Time 5.00 hour
fired; ASTM C113
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Al2O3 28 %28 %after firing
CaO 11.5 %11.5 %after firing
Fe2O3 2.6 %2.6 %after firing
K2O+Na2O 2.3 %2.3 %Na2O & K2O
MgO 0.70 %0.70 %after firing
SiO2 53.5 %53.5 %after firing
TiO2 1.2 %1.2 %after firing
 
Descriptive Properties
Placement, average (kg)35to place 1m3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6308 / 203092

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.