MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Moso Bamboo
Categories: Wood and Natural Products; Wood

Material Notes: From China; most common Bamboo species used in manufactured bamboo products. Relatively fine grain and relatively small nodes. A modest increase in mechanical properties occurs toward the outside of the plant (the culm wall).

Key Words: Phyllostachys edulis; Giant Timber Bamboo
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.600 g/ccat 10.3% moisture (equilibrium at 65% RH and 20°C)
Moisture Absorption at Equilibrium 10.3 %65% RH
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 5500 NInternode; Inside; Janka Hardness
 5900 NInternode; Outside; Janka Hardness
 6200 NNode; Inside; Janka Hardness
 7500 NNode; Outside; Janka Hardness
Modulus of Rupture 0.0800 GPaInternode; Inside; 4 point bend test
 0.0810 GPaInternode; Outside; 4 point bend test
 0.0810 GPaNode; Inside; 4 point bend test
 >= 0.0820 GPa5th percentile; 4 point bend test
 0.0910 GPaNode; Outside; 4 point bend test
Flexural Modulus >= 9.00 GPa5th percentile; 4 point bend test
 10.6 GPaNode; Inside; 4 point bend test
 11.0 GPaNode; Outside; 4 point bend test
 11.5 GPaInternode; Outside; 4 point bend test
 11.8 GPaInternode; Inside; 4 point bend test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Guadua Bamboo
American Red Oak Wood
Tropical Balsa Wood
American Balsa Wood
American White Oak Wood

PTSAV901 / 146104

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.