MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex Q 302B Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex Q 302 B is a reactor TPO (thermoplastic polyolefin) manufactured using LyondellBasell's proprietary Catalloy process technology. It resists gas fading and brings a warm and sensual feel. Part of a family of polymers with a soft, velvety texture, Adflex Q 302 B resin enables packagers to give their products a distinct edge over conventional plastics.  Bottles blow molded from Adflex Q 302 B resin convey an upscale, quality image that enhances point of purchase appeal.  The texture is also useful for applications requiring a no-slip surface, such as shower soaps and lotions. Applications: Bottles For Consumer Goods, Soft Touch Applications, Sports, Leisure & Toys.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccMethod A; ISO 1183-1
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
@Time 15.0 sec
ISO 868
Tensile Strength at Break 10.0 MPaISO 527-1,-2
Tensile Strength, Yield 8.50 MPaISO 527-1,-2
Elongation at Break 500 %ISO 527-1,-2
Elongation at Yield 37 %ISO 527-1,-2
Flexural Modulus 350 MPaISO 178
Charpy Impact, Notched 3.20 kJ/m²
@Temperature -40.0 °C
failure mode: complete break; ISO 179
 70.0 kJ/m²
@Temperature 23.0 °C
failure mode-partial break; ISO 179
 98.0 kJ/m²
@Temperature -20.0 °C
failure mode-partial break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 52.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 67.0 °CA50; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 96 %
@Thickness 1.14 mm
ASTM D1003
Gloss 49 %
@Thickness 1.14 mm
@60°; ASTM D2457
 
Descriptive Properties
Processing MethodExtrusion Blow Molding; Injection Blow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
Avient OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE)
Innospec FLEXAREN® 14001 EVA-Copolymer
ExxonMobil LD 70013.BA Low Density Polyethylene Resin (European Grade)
ExxonMobil LD 22014.BA Low Density Polyethylene Resin (European Grade)

PEQT7008 / 218647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.