MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Artificial Flowers
  • Carpet Backing
  • Compounding
  • Injection Molding
  • Masterbatch Base Resin

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc0.0330 lb/in³ExxonMobil method
Melt Flow 70 g/10 min70 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3838ISO 868
Tensile Strength at Break 6.89 MPa1000 psiISO 527-2/1A/50
Elongation at Break 150 %150 %ISO 527-2/1A/50
Tensile Modulus 0.103 GPa15.0 ksiISO 527-2/1A/1
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 101 °C<= 214 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 75.0 °C167 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Lucalen A2920M Low Density Polyethylene
ExxonMobil LDPE LD 650 Low Density Polyethylene Resin (European Grade)
ExxonMobil LD 509.48 Compounding Resin
ExxonMobil LDPE LD 655 Low Density Polyethylene Resin (European Grade)
Celanese 191A LDPE polymer for adhesives, automotive and compounds

PEX99287 / 175523

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.