MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP5341E1 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: A low melt flow rate that provides high melt strength and resistance to softening at elevated temperature.

Availability: North America

Features:

  • Low Flow
Uses:
  • Automotive Applications
  • Industrial Applications
Processing Method: Blow Molding, Compounding, Injection Molding, Sheet Extrusion and Thermoforming

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 0.83 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4640 psi2.0 in/min; ASTM D638
Elongation at Yield 13 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 172000 psi0.05 in/min; ASTM D790A
 201000 psi0.5 in/min; ASTM D790B
Izod Impact, Notched 0.980 ft-lb/inASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 183 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming
ExxonMobil PP1074KNE1 Polypropylene Homopolymer
ExxonMobil Exceed™ PP7815E1 Polypropylene Homopolymer
ExxonMobil Exceed™ PP9122 Polypropylene Homopolymer
ExxonMobil Exceed™ PP9513 Polypropylene Homopolymer

PEX99400 / 175636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.