Product Description: A nucleated, medium flow rate homopolymer resin with mold release and anti-static properties. It is suitable for general purpose injection molding. Availability: North America Features: - Autoclave Sterilizable
- Ethylene Oxide Sterilizable
- Good Creep Resistance
- Good Mold Release
- Good Stiffness
- Steam Sterilizable
Uses: - Bottles
- Caps
- Closures
- Consumer Applications
- Packaging
Processing Method: Injection MoldingInformation provided by ExxonMobil |