MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper, UNS C66400, O60 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Applications: spring washers, switchblades, fuse clips, contact springs, socket contacts, connectors, terminals.

Key Words: Cobron
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.74 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 435 MPa
Tensile Strength, Yield 310 MPa
@Strain 0.2 %
Elongation at Break 25 %in 50 mm
Modulus of Elasticity 112 GPa
Fatigue Strength 165 MPa
@# of Cycles 1.00e+8
Reverse Bending
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000575 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 116 W/m-K
Melting Point 1035 - 1055 °C
Solidus 1035 °C
Liquidus 1055 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.050 %
Cobalt, Co 0.30 - 0.70 %
Copper, Cu 86.5 %
Iron, Fe 1.3 - 1.7 %
Lead, Pb <= 0.015 %
Manganese, Mn <= 0.050 %
Nickel, Ni <= 0.050 %
Phosphorus, P <= 0.020 %
Silicon, Si <= 0.050 %
Silver, Ag <= 0.050 %
Tin, Sn <= 0.050 %
Zinc, Zn 11 - 12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C66400, H01 Temper
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO70 Temper flat products
Low-silicon bronze B, UNS C65100, OSO35 Temper rod
Copper, UNS C66400, H02 Temper
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO35 Temper flat products

MC66400b1 / 11671

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.