System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Copper, UNS C66400, O60 Temper
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
Material Notes:
Applications:
spring washers, switchblades, fuse clips, contact springs, socket contacts, connectors, terminals.
Key Words:
Cobron
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
8.74
g/cc
0.316
lb/in³
Mechanical Properties
Metric
English
Comments
Tensile Strength, Ultimate
435
MPa
63100
psi
Tensile Strength, Yield
310
MPa
@Strain 0.2 %
45000
psi
@Strain 0.2 %
Elongation at Break
25 %
25 %
in 50 mm
Modulus of Elasticity
112
GPa
16200
ksi
Fatigue Strength
165
MPa
@# of Cycles 1.00e+8
23900
psi
@# of Cycles 1.00e+8
Reverse Bending
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00000575
ohm-cm
@Temperature 20.0 °C
0.00000575
ohm-cm
@Temperature 68.0 °F
Thermal Properties
Metric
English
Comments
Thermal Conductivity
116
W/m-K
805
BTU-in/hr-ft²-°F
Melting Point
1035
-
1055
°C
1895
-
1931
°F
Solidus
1035
°C
1895
°F
Liquidus
1055
°C
1931
°F
Component Elements Properties
Metric
English
Comments
Aluminum, Al
<= 0.050 %
<= 0.050 %
Cobalt, Co
0.30 - 0.70 %
0.30 - 0.70 %
Copper, Cu
86.5 %
86.5 %
Iron, Fe
1.3 - 1.7 %
1.3 - 1.7 %
Lead, Pb
<= 0.015 %
<= 0.015 %
Manganese, Mn
<= 0.050 %
<= 0.050 %
Nickel, Ni
<= 0.050 %
<= 0.050 %
Phosphorus, P
<= 0.020 %
<= 0.020 %
Silicon, Si
<= 0.050 %
<= 0.050 %
Silver, Ag
<= 0.050 %
<= 0.050 %
Tin, Sn
<= 0.050 %
<= 0.050 %
Zinc, Zn
11 - 12 %
11 - 12 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Copper, UNS C66400, H01 Temper
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO70 Temper flat products
Low-silicon bronze B, UNS C65100, OSO35 Temper rod
Copper, UNS C66400, H02 Temper
Herculoy®, High-Silicon Bronze A, UNS C65500, OSO35 Temper flat products
MC66400b1 / 11671
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.