MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Blue River Coatings Steel Seal Primer
Categories: Polymer; Adhesive; Thermoset

Material Notes: BLUE RIVER COATINGS STEEL SEAL PRIMER is a high quality, single component primer, not requiring any catalyzing agent. STEEL SEAL PRIMER is designed for dip coaters who need a quick, fast drying paint for corrosion resistance and high gloss. STEEL SEAL PRIMER dries in about 6-8 minutes @ 70°F and 50% humidity. STEEL SEAL PRIMER offers good coverage and durability, as well as being a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS STEEL SEAL PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent dip coating
  • Good hardness/impact resistance
  • Good mar and abrasion resistance
  • Solvent resistant
  • Can be applied in a wide variety of temperature and humidity conditions without the use of retarders
  • Distilled water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • 80% gloss on 60° glossometer
  • Air dry or force curing preferred
  • Can be oven baked
  • Wide range of colors
  • Coating will not flash rust on bare metal
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Uses

  • Steel
  • Aluminum
  • Metal Pipe
  • Salt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654.

  • 200 hours
  • Scribed – 1/16” dense #4. Moderate rust rundown OK – moderate rust rundown
  • Unscribed – OK – moderate rust rundown
  • Information provided by Blue River Coatings

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity >= 1.00 g/cc>= 1.00 g/cc
    Density 1.03 g/cc0.0372 lb/in³
    Solids Content 32 %32 %by volume
     35 %35 %by weight
    Volatile Organic Compounds (VOC) Content 60 g/l60 g/l
    pH 7.0 - 8.57.0 - 8.5
     
    Mechanical PropertiesMetricEnglishComments
    Impact Test 11.3 J8.33 ft-lbReverse/direct on steel
     
    Thermal PropertiesMetricEnglishComments
    Boiling Point 169 °C336 °F
    Flash Point 65.6 °C150 °F
     
    Processing PropertiesMetricEnglishComments
    Cure Time  1.00 min
    @Temperature 75.0 °C
    0.0167 hour
    @Temperature 167 °F
    Dry to handle, at 50% humidity and 75°C
     4.02 min
    @Temperature 75.0 °C
    0.0670 hour
    @Temperature 167 °F
    Dust Free, at 50% humidity
     4.02 - 4.98 min
    @Temperature 75.0 °C
    0.0670 - 0.0830 hour
    @Temperature 167 °F
    Recoat, at 50% humidity
    Shelf Life 12.0 Month12.0 Month
     
    Descriptive Properties
    Evaporation rateSlower than ether
    Theoretical Coverage514 ft2 at 1 mil
    Vapor DensityHeavier than air

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ASTM A228 Steel (UNS K08500)
    Aperam Resistohm® 140 Resistant Alloys Iron-Chromium-Aluminium Alloy
    Von Roll Isola IMI Varnish 74035 Solventless Epoxy Varnish for Electrical Insulation
    VICTREX™ PEEK 150G903 Black Polyetheretherketone, Unreinforced
    Mitsubishi Chemical Advanced Materials Ketron™ Sterra™ HPV PEEK Recycled poly-ether-ether-ketone

    WBLUER03 / 74602

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.