MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Assab Steels CARMO Cold Work Steel
Categories: Metal; Ferrous Metal; Chrome-moly Steel; Tool Steel; Cold Work Steel

Material Notes: CARMO is a high-strength, flame-induction and through hardening steel delivered prehardened to 240-270 HB.
The surface of the steel can be flame-hardened without water cooling to a hardness of 58±2 HRC. The depth of hardness is normally 4-5 mm and the hardened and tempered matrix is a good base for the flame-hardened layer. The steel can be easily repair welded and has a high wear resistance similar to that of A2. The toughness of CARMO is much better than that for the steel types A2 and D2.

CARMO is a cold work tool steel which has been developed together with the automotive industry. Its analysis has been balanced to give one universal tool steel for car body dies instead of the several steel grades (flame hardening and through hardening grades) which are normally used. The steel can be used in the flame-hardened or in the through-hardened condition for blanking and forming of both car body parts (thin sheet) or structural parts (thicker sheet).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 4343Surface hardness. 600°C Tempering temperature, TA = 960°C
 5555Surface hardness. 400°C Tempering temperature, TA = 960°C
 5858At 900°C Austenitizing temperature during hardening
 6060Core hardness in air cooling for a diameter of 100 mm.
 6262Core hardness in air cooling for a diameter of 50 mm.
 6363At 960°C Austenitizing temperature during hardening
 6363Surface hardness. 100°C Tempering temperature, TA = 960°C
 6363Core hardness in air cooling for a diameter of 1-20 mm.
 6565At 1025°C Austenitizing temperature during hardening
Tensile Strength, Ultimate 870 MPa126000 psiRm, @RT, 270 HB.
Tensile Strength, Yield 670 MPa97200 psiRp0.2, @RT, 270 HB.
Elongation at Break 15 %15 %
Reduction of Area 50 %50 %
Impact Test 125 J92.2 ft-lbRT. 450°C tempering temp. Specimen size: 7x10x55 mm unnotched. Hardened at 960°C. Quenched in air. Tempered twice
 200 J148 ft-lbRT. 250°C tempering temp. Specimen size: 7x10x55 mm unnotched. Hardened at 960°C. Quenched in air. Tempered twice
 260 J192 ft-lbRT. 600°C tempering temp. Specimen size: 7x10x55 mm unnotched. Hardened at 960°C. Quenched in air. Tempered twice
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.3 µm/m-°C
@Temperature 20.0 - 200 °C
6.83 µin/in-°F
@Temperature 68.0 - 392 °F
Hardened and tempered to 56 HRC
 13.3 µm/m-°C
@Temperature 20.0 - 400 °C
7.39 µin/in-°F
@Temperature 68.0 - 752 °F
Hardened and tempered to 56 HRC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.60 %0.60 %
Chromium, Cr 4.5 %4.5 %
Iron, Fe 93.05 %93.05 %
Manganese, Mn 0.80 %0.80 %
Molybdenum, Mo 0.50 %0.50 %
Silicon, Si 0.35 %0.35 %
Vanadium, V 0.20 %0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Assab Steels CALMAX Plastic Mold Material
EDRO #7 Shock Resistant S7 Tool Steel
ASTM A213 T5 5Cr-0.5Mo STEEL TUBES FOR BOILERS AND HEAT EXCHANGERS (STBA 25)
ASTM A387 Alloy Steel, Grade 5, Class 2
Bohler-Uddeholm UDDEHOLM Carmo Granshots Tool Steel Foundry Meltstock

NASSAB09 / 15027

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.