MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik TEGOMER® AntiScratch 100 Polyolefin compound
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product description: TEGOMER® AntiScratch 100 is a siloxane polyolefin compound delivered in pelletized form.

Application:

  • TEGOMER® AntiScratch 100 is recommended to be used in polyolefin compounds to guarantee permanent scratch resistance.
  • TEGOMER® AntiScratch 100 is also suitable for PP/TPO systems used for interior or exterior car application.
  • TEGOMER® AntiScratch 100 is used for unfilled PP compounds as often used for domestic appliances.
  • TEGOMER® AntiScratch 100 can be applied in alloys based on polyolefin with polar thermo-plastic materials such as PBT or PA.
Benefits: TEGOMER® AntiScratch 100 is a none migrative additive for the improvement of permanent, long-term scratch resistance. TEGOMER® AntiScratch 100 has superior scratch performance even after elevated temperature storing and UV-aging and shows no fogging. TEGOMER® AntiScratch 100 is highly effective and does not have to be combined with amides to achieve high scratch resistance. TEGOMER® AntiScratch 100 works in a wide range of talc filling as it is typical for interior and exterior automotive application with 10 – 40 % talc filling. TEGOMER® AntiScratch 100 does not influence the gloss of the polyolefin compound. TEGOMER® AntiScratch 100 is suitable for thermoplastic polyolefins with other inorganic fillers, e. g. wollastonite as used for light weight automotive developments.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.225 - 0.325 g/cc0.00813 - 0.0117 lb/in³
Melt Flow >= 100 g/10 min
@Load 2.16 kg,
Temperature 230 °C
>= 100 g/10 min
@Load 4.76 lb,
Temperature 446 °F
 
Descriptive Properties
Appearancewhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Excelite Plastic AS-200 Anti-scratch polycarbonate
Overview of materials for Polycarbonate, Impact Modified
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
LG Chemical XG569C MABS, Anti-Scratch, High Gloss
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets

PEVONIL572 / 196776

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.