MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Feature: Injection Molding, Anti-Scratch, High Impact, High Flow

Application: LCD TV Stand Base, Audio/Video Housing

CAS No. 9010-94-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D792
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
0.30 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 22 g/10 min
@Load 10.0 kg,
Temperature 220 °C
22 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Yield 49.0 MPa
@Thickness 3.20 mm
7110 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 30 %
@Thickness 3.20 mm
30 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 6.0 %
@Thickness 3.20 mm
>= 6.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Yield Strength 82.4 MPa
@Thickness 3.20 mm
11900 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.89 GPa
@Thickness 3.20 mm
420 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  1.77 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
3.31 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 1.77 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
3.31 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched  0.981 J/cm
@Thickness 6.40 mm,
Temperature -20.0 °C
1.84 ft-lb/in
@Thickness 0.252 in,
Temperature -4.00 °F
ASTM D256
 0.981 J/cm
@Thickness 3.20 mm,
Temperature -20.0 °C
1.84 ft-lb/in
@Thickness 0.126 in,
Temperature -4.00 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi)  87.0 °C
@Thickness 6.40 mm
189 °F
@Thickness 0.252 in
Unannealed; ASTM D648
 87.0 °C
@Thickness 3.20 mm
189 °F
@Thickness 0.126 in
Unannealed; ASTM D648
 91.0 °C
@Thickness 6.40 mm
196 °F
@Thickness 0.252 in
ASTM D648
 91.0 °C
@Thickness 3.20 mm
196 °F
@Thickness 0.126 in
ASTM D648
Flammability, UL94  HB
@Thickness >=1.60 mm
HB
@Thickness >=0.0630 in
 HB
@Thickness >=3.20 mm
HB
@Thickness >=0.126 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °FInjection Molding
Middle Barrel Temperature 180 - 200 °C356 - 392 °FInjection Molding
Front Barrel Temperature 190 - 210 °C374 - 410 °FInjection Molding
Nozzle Temperature 200 - 220 °C392 - 428 °FInjection Molding
Melt Temperature 200 - 230 °C392 - 446 °FInjection Molding
Mold Temperature 40.0 - 60.0 °C104 - 140 °FInjection Molding
Drying Temperature 80.0 - 90.0 °C176 - 194 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HF-350 ABS, High Flow, High Impact
LG Chemical HF-380 ABS, High Flow, High Impact
Aclo Accucomp ABS ABS803L Medium Impact Grade
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene
Arkema Platamid® H 2519 Pellets Polyamide

PLAY029 / 148037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.