MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Seashell Technology Silver Nanowires
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Seashell Technology provides silver nanowire populations in isopropyl alcohol suspensions in several varieties: 1) AgNW-60 (ave dia. = 60 nm, and ave. length = 10 um); 2) AgNW-115 (ave dia. = 115 nm, and ave. length = 30 um); 3) Custom dimensions; 4) Custom carrier fluids (water, toluene, ethanol, others)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.800 - 1.40 g/cc
Solids Content 0.10 - 100 %
Filler Content 0.10 - 5.0 %Silver (Ag)
Particle Size 25 µm
Viscosity 10 - 10000 cP
Thickness 0.500 - 50.0 microns
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00010 - 0.0010 ohm-cm
Surface Resistivity per Square 1.0 - 50 ohm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 50 - 92 %
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 3600 sec
 
Descriptive Properties
Adhesiongood
Binder SystemNone (solvent dispersion) or Epoxy
Conductive Filler TypeSilver (Ag)
Material TypeDispersion
Solvent SystemIsopropyl Alcohol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Elements Carbon Nanotubes
American Elements Silver Nanoparticles
NanoAmor 90% Regular Single Walled Carbon Nanotubes
NanoAmor 95%, OD/ID/L: < 8/2-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
Evonik VP Disp. ITO IR5 Coating

PFLEXCM43 / 179445

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.