MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Elements Silver Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Silver (Ag) Nanoparticles, nanodots or nanopowder are spherical or flake high surface area metal particles. Nanoscale Silver Particles are typically 1 - 40 nanometers (nm) with specific surface area (SSA) in the 1 – 1 m 2 /g range and also available as flakes with an average particle size of 2-10 micron range with a specific surface area of approximately 1 m 2 /g. Nano Silver Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for silver nanocrystals and flakes include as an anti-microbial, anti-biotic and anti-fungal agent when incorporated in coatings, nanofiber, first aid bandages, plastics, soap and textiles, in treatment of certain viruses, in self cleaning fabrics, as a conductive filler and in nanowire and certain catalyst applications. See the Silver Nanoparticles product data sheet.

Key Words: Formula: Ag; CAS Number: 7440-22-4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 10.49 g/cc0.3790 lb/in³
Particle Size 0.0010 - 0.040 µm0.0010 - 0.040 µm
 2.0 - 10 µm2.0 - 10 µm
Specific Surface Area 1.0 m²/g1.0 m²/g
 1.0 m²/g1.0 m²/g
Molecular Weight 107.87 g/mol107.87 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 961.78 °C1763.2 °F
Boiling Point 2162 °C3924 °F
 
Descriptive Properties
AppearanceSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seashell Technology Silver Nanowires
NanoAmor 95%, OD/ID/L: < 8/2-5 nm/0.5-2 um Short Multi-Walled Carbon Nanotubes
Evonik VP Disp. ITO TC8 Coating
Evonik VP Disp. ITO IR5 Coating
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver

EJAMER78 / 5561

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.