MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet is capable of maintenance free operation up to 218°C (425°F). Applications include Fine and specialty chemical processing, pharmaceutical production, and environmental test chambers

Information provided by Paratherm Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.30 lb/gal
@Temperature 218 °C
 5.60 lb/gal
@Temperature 177 °C
 6.10 lb/gal
@Temperature 121 °C
 6.50 lb/gal
@Temperature 65.6 °C
 6.80 lb/gal
@Temperature 23.9 °C
 6.90 lb/gal
@Temperature 15.6 °C
 7.30 lb/gal
@Temperature -17.8 °C
 7.40 lb/gal
@Temperature -45.6 °C
 7.70 lb/gal
@Temperature -73.3 °C
Viscosity 0.24 cP
@Temperature 218 °C
 0.28 cP
@Temperature 177 °C
 0.35 cP
@Temperature 121 °C
 0.51 cP
@Temperature 65.6 °C
 1.0 cP
@Temperature -17.8 °C
 1.0 cP
@Temperature 23.9 °C
 2.0 cP
@Temperature -45.6 °C
 5.0 cP
@Temperature -73.3 °C
Viscosity Measure 0.38 cSt
@Temperature 218 °C
 0.42 cSt
@Temperature 177 °C
 0.48 cSt
@Temperature 121 °C
 0.65 cSt
@Temperature 65.6 °C
 0.94 cSt
@Temperature 23.9 °C
 1.5 cSt
@Temperature -17.8 °C
 2.5 cSt
@Temperature -45.6 °C
 5.5 cSt
@Temperature -73.3 °C
Molecular Weight 130 g/molaverage
Vapor Pressure 28.0 torr
@Temperature 65.6 °C
 208 torr
@Temperature 121 °C
 719 torr
@Temperature 177 °C
 1074 torr
@Temperature 218 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.3e+11 ohm-cm
Dielectric Constant 2.59
@Frequency 1000 Hz
ASTM D924-04
Dielectric Breakdown 36110 V
@Thickness 2.54 mm
ASTM D1816-04
Dissipation Factor 0.00145
@Frequency 1000 Hz
ASTM D924-04
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 82.2 cal/g
Specific Heat Capacity 0.380 BTU/lb-°F
@Temperature -73.3 °C
 0.400 BTU/lb-°F
@Temperature -45.6 °C
 0.430 BTU/lb-°F
@Temperature -17.8 °C
 0.460 BTU/lb-°F
@Temperature 23.9 °C
 0.500 BTU/lb-°F
@Temperature 65.6 °C
 0.550 BTU/lb-°F
@Temperature 121 °C
 0.600 BTU/lb-°F
@Temperature 177 °C
 0.630 BTU/lb-°F
@Temperature 218 °C
Thermal Conductivity 0.864 BTU-in/hr-ft²-°F
@Temperature 218 °C
 0.888 BTU-in/hr-ft²-°F
@Temperature 177 °C
 0.924 BTU-in/hr-ft²-°F
@Temperature 121 °C
 0.948 BTU-in/hr-ft²-°F
@Temperature 65.6 °C
 0.972 BTU-in/hr-ft²-°F
@Temperature 23.9 °C
 0.996 BTU-in/hr-ft²-°F
@Temperature -17.8 °C
 1.008 BTU-in/hr-ft²-°F
@Temperature -45.6 °C
 1.02 BTU-in/hr-ft²-°F
@Temperature -73.3 °C
Boiling Point 182 °C
Maximum Service Temperature, Air 425 °F
 550 °Fmax. recommended film temperature
Minimum Service Temperature, Air -127 °F
Flash Point >= 104 °Fclosed cup; ASTM D56
Ignition Temperature >= 430 °FAutoignition; < 10 sec delay
 
Descriptive Properties
Appearancewater white
Chemistrysynthetic hydrocarbon blend
Odorsweet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid

WPAR03x / 160263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.