MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Paratherm Corporation Paratherm™ LR Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam heaters and down to a -58°F surface temperature in direct-expansion exchangers.

Information provided by Paratherm Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.611 g/cc
@Temperature 232 °C
0.0221 lb/in³
@Temperature 450 °F
 0.647 g/cc
@Temperature 177 °C
0.0234 lb/in³
@Temperature 350 °F
 0.695 g/cc
@Temperature 121 °C
0.0251 lb/in³
@Temperature 250 °F
 0.731 g/cc
@Temperature 65.6 °C
0.0264 lb/in³
@Temperature 150 °F
 0.755 g/cc
@Temperature 23.9 °C
0.0273 lb/in³
@Temperature 75.0 °F
 0.767 g/cc
@Temperature 15.6 °C
0.0277 lb/in³
@Temperature 60.0 °F
 0.791 g/cc
@Temperature -17.8 °C
0.0286 lb/in³
@Temperature 0.000 °F
 0.815 g/cc
@Temperature -45.6 °C
0.0294 lb/in³
@Temperature -50.0 °F
 0.827 g/cc
@Temperature -73.3 °C
0.0299 lb/in³
@Temperature -100 °F
Viscosity  0.18 cP
@Temperature 232 °C
0.18 cP
@Temperature 450 °F
 0.26 cP
@Temperature 177 °C
0.26 cP
@Temperature 350 °F
 0.42 cP
@Temperature 121 °C
0.42 cP
@Temperature 250 °F
 0.80 cP
@Temperature 65.6 °C
0.80 cP
@Temperature 150 °F
 1.5 cP
@Temperature 23.9 °C
1.5 cP
@Temperature 75.0 °F
 5.0 cP
@Temperature -17.8 °C
5.0 cP
@Temperature 0.000 °F
 16 cP
@Temperature -45.6 °C
16 cP
@Temperature -50.0 °F
 154 cP
@Temperature -73.3 °C
154 cP
@Temperature -100 °F
Viscosity Measure  0.30 cSt
@Temperature 232 °C
0.30 cSt
@Temperature 450 °F
 0.40 cSt
@Temperature 177 °C
0.40 cSt
@Temperature 350 °F
 0.61 cSt
@Temperature 121 °C
0.61 cSt
@Temperature 250 °F
 1.0 cSt
@Temperature 65.6 °C
1.0 cSt
@Temperature 150 °F
 2.0 cSt
@Temperature 23.9 °C
2.0 cSt
@Temperature 75.0 °F
 5.9 cSt
@Temperature -17.8 °C
5.9 cSt
@Temperature 0.000 °F
 19 cSt
@Temperature -45.6 °C
19 cSt
@Temperature -50.0 °F
 185 cSt
@Temperature -73.3 °C
185 cSt
@Temperature -100 °F
Molecular Weight 160 g/mol160 g/molaverage
Vapor Pressure  0.0400 bar
@Temperature 107 °C
30.0 torr
@Temperature 225 °F
 0.0667 bar
@Temperature 121 °C
50.0 torr
@Temperature 250 °F
 0.108 bar
@Temperature 135 °C
81.0 torr
@Temperature 275 °F
 0.193 bar
@Temperature 149 °C
145 torr
@Temperature 300 °F
 0.500 bar
@Temperature 177 °C
375 torr
@Temperature 350 °F
 1.04 bar
@Temperature 204 °C
780 torr
@Temperature 400 °F
 1.25 bar
@Temperature 218 °C
938 torr
@Temperature 425 °F
 1.421 bar
@Temperature 232 °C
1066 torr
@Temperature 450 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.84e+14 ohm-cm1.84e+14 ohm-cm
Dielectric Constant 2.03
@Frequency 1000 Hz
2.03
@Frequency 1000 Hz
ASTM D924-04
Dielectric Breakdown 22150 V
@Thickness 2.54 mm
22150 V
@Thickness 0.100 in
ASTM D1816-04
Dissipation Factor 0.000010
@Frequency 1000 Hz
0.000010
@Frequency 1000 Hz
ASTM D924-04
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 262 J/g113 BTU/lb
Specific Heat Capacity  1.63 J/g-°C
@Temperature -73.3 °C
0.390 BTU/lb-°F
@Temperature -100 °F
 1.76 J/g-°C
@Temperature -45.6 °C
0.420 BTU/lb-°F
@Temperature -50.0 °F
 1.84 J/g-°C
@Temperature -17.8 °C
0.440 BTU/lb-°F
@Temperature 0.000 °F
 2.01 J/g-°C
@Temperature 23.9 °C
0.480 BTU/lb-°F
@Temperature 75.0 °F
 2.18 J/g-°C
@Temperature 65.6 °C
0.520 BTU/lb-°F
@Temperature 150 °F
 2.38 J/g-°C
@Temperature 121 °C
0.570 BTU/lb-°F
@Temperature 250 °F
 2.59 J/g-°C
@Temperature 177 °C
0.620 BTU/lb-°F
@Temperature 350 °F
 2.80 J/g-°C
@Temperature 232 °C
0.670 BTU/lb-°F
@Temperature 450 °F
Thermal Conductivity  0.131 W/m-K
@Temperature 232 °C
0.912 BTU-in/hr-ft²-°F
@Temperature 450 °F
 0.137 W/m-K
@Temperature 177 °C
0.948 BTU-in/hr-ft²-°F
@Temperature 350 °F
 0.142 W/m-K
@Temperature 121 °C
0.984 BTU-in/hr-ft²-°F
@Temperature 250 °F
 0.147 W/m-K
@Temperature 65.6 °C
1.02 BTU-in/hr-ft²-°F
@Temperature 150 °F
 0.1504 W/m-K
@Temperature 23.9 °C
1.044 BTU-in/hr-ft²-°F
@Temperature 75.0 °F
 0.1539 W/m-K
@Temperature -17.8 °C
1.068 BTU-in/hr-ft²-°F
@Temperature 0.000 °F
 0.1574 W/m-K
@Temperature -45.6 °C
1.092 BTU-in/hr-ft²-°F
@Temperature -50.0 °F
 0.1591 W/m-K
@Temperature -73.3 °C
1.104 BTU-in/hr-ft²-°F
@Temperature -100 °F
Boiling Point 202 °C396 °F
Maximum Service Temperature, Air 232 °C450 °F
 260 °C500 °Fmax. recommended film temperature
Minimum Service Temperature, Air -50.0 °C-58.0 °F
Flash Point >= 54.4 °C>= 130 °Fclosed cup; ASTM D56
Ignition Temperature >= 260 °C>= 500 °FAutoignition; < 10 sec delay
 
Descriptive Properties
Appearancewater white
Feedstockhydrocarbon
Odornone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid

WPAR03m / 160262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.