MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Gichem GIPLENE DX04/V2 Polypropylene - Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: PP self-extinguishing, class V2, excellent mechanical properties. Medium injection speed.

Information provided by GICHEM Gruppo Industriale Chimico

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccASTM D792
Water Absorption 0.020 %ASTM D570
Linear Mold Shrinkage 0.011 - 0.014 cm/cmASTM D955
Melt Flow 10 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Yield 40 %ASTM D638
Flexural Modulus 1.80 GPaASTM D790
Izod Impact, Notched 25.0 J/mASTM D256
 20.0 J/m
@Temperature 0.000 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CASTM D648
Vicat Softening Point 92.0 °CASTM D1525/A
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
 V-2
@Thickness 0.800 mm
Flammability Test 125[°C] Bilia; IEC 331
Oxygen Index 26 %ASTM D2863
Glow Wire Test 960 °CIEC 695-2-1
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 180 - 200 °C
Mold Temperature 60.0 °C
Drying Temperature 60.0 °C2 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SPS Guang Zhou SAMAT™ 666(f1) Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000C Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000AC Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000A Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 168(f1) Flame-retarded Polypropylene

PGICH20 / 41837

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.