MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gichem GIPLENE DX04/V2 Polypropylene - Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: PP self-extinguishing, class V2, excellent mechanical properties. Medium injection speed.

Information provided by GICHEM Gruppo Industriale Chimico

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %ASTM D570
Linear Mold Shrinkage 0.011 - 0.014 cm/cm0.011 - 0.014 in/inASTM D955
Melt Flow 10 g/10 min10 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Elongation at Yield 40 %40 %ASTM D638
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched 0.250 J/cm0.468 ft-lb/inASTM D256
 0.200 J/cm
@Temperature 0.000 °C
0.375 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FASTM D648
Vicat Softening Point 92.0 °C198 °FASTM D1525/A
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
Flammability Test 125125[°C] Bilia; IEC 331
Oxygen Index 26 %26 %ASTM D2863
Glow Wire Test 960 °C1760 °FIEC 695-2-1
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 180 - 200 °C356 - 392 °F
Mold Temperature 60.0 °C140 °F
Drying Temperature 60.0 °C140 °F2 hours

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SPS Guang Zhou SAMAT™ 666(f1) Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000C Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000AC Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 5000A Flame-retarded Polypropylene
SPS Guang Zhou SAMAT™ 168(f1) Flame-retarded Polypropylene

PGICH20 / 41837

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.