MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Permabond LH054 Anaerobic Threadsealant
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with metal parts (as in a threaded pipe joint). The product is instant sealing with full cure occurring in 12-16 hours. The permanent seal is inert to hydrocarbons (gasoline, diesel fuel), most acids, solvents and steam.

Permabond® LH054 seals iron, copper or brass pipe and is designed to obtain more complete cure on less active surfaces such as stainless steel and aluminum.

The product is available in a brush-top dispenser. It is applied onto the first few threads, assembled and tightened with a wrench. Instant sealability of 500 psi is obtained, but final adjustment can be made up to several hours after assembly.

Features & Benefits:

  • Easy to use and apply
  • Directional freedom
  • Does not contain solvents
  • Excellent chemical and temperature resistance
  • Cures at room temperature
  • Will not shred, tear or cause blockages

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccUncured
Viscosity 260000 cP
@Temperature 25.0 °C
Uncured
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 7.00 MPasteel collar and pin shear; ISO 10123
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
Thermal Conductivity 0.190 W/m-K
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 16.0 hour
@Temperature 23.0 °C
M10 steel, handling strength
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhiteUncured
Maximum Gap Fill (mm)0.5
Strength Retention20% at 200°CRelative to 0°C
 60% at 150°CRelative to 0°C
 85% at 100°CRelative to 0°C
 93% at 50°CRelative to 0°C
Torque Strength (N m)2M10 steel, prevail
 3M10 steel, break
UV FluorescenceNoUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERMA14 / 56122

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.