MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical LUCON CP6052 PC/ABS+CNT  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description Injection Molding Grade, PC/ABS+CNT, Electrostatic Dissipation, Low Surface Resistivity, Improved Impact Strength

Application: Laser diode Tray, ATM parts, Telecommunication Station Housing,

CAS No. 103598-77-2, 9003-56-9, 181028-79-5 and 1333-86-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.24 g/cc1.24 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 250 °C
7.0 g/10 min
@Load 22.0 lb,
Temperature 482 °F
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.7 MPa
@Thickness 3.20 mm
9250 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break >= 10 %
@Thickness 3.20 mm
>= 10 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 98.1 MPa
@Thickness 6.40 mm
14200 psi
@Thickness 0.252 in
15mm/min; ASTM D790
Flexural Modulus 2.94 GPa
@Thickness 6.40 mm
427 ksi
@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched 0.441 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
0.827 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 - 1.00e+7 ohm10000 - 1.00e+7 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C
@Thickness 6.40 mm
243 °F
@Thickness 0.252 in
ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 300 °C500 - 572 °FInjection Molding
Middle Barrel Temperature 270 - 310 °C518 - 590 °FInjection Molding
Front Barrel Temperature 270 - 310 °C518 - 590 °FInjection Molding
Nozzle Temperature 270 - 310 °C518 - 590 °FInjection Molding
Melt Temperature 270 - 310 °C518 - 590 °FInjection Molding
Mold Temperature 60.0 - 80.0 °C140 - 176 °FInjection Molding
Drying Temperature 70.0 - 80.0 °C158 - 176 °FInjection Molding
Dry Time 5.00 - 7.00 hour5.00 - 7.00 hourInjection Molding
Back Pressure 0.000 - 1.96 MPa0.000 - 284 psiInjection Molding
Screw Speed 40 - 60 rpm40 - 60 rpmInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ABS 9401 Injection Molding Grade, Ultra High Impact
The NanoSteel® Company SHS 9700 Steel Alloy, Wear Plate
SSAB Tunnplat Domex® Wear Steel Sheet
SSAB Tunnplat Domex® 700MC HSLA Steel
SSAB Tunnplat Domex® 500MC HSLA Steel

PLAY272 / 148282

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.