MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Entec Enflex® EA3720 Styrenic Block, TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Product Description: 20 Shore A TPE (Styrenic Block Copolymer based) available in black and natural for injection molding and extrusion applications. This grade offers soft/tactile feel and adhesion (overmolding or co-extrusion) to ABS, PC and HIPS/PS

Availability: North America

Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Processability; High Elasticity; Oil Resistant; Ozone Resistant; Recyclable Material; Soft; Solvent Resistant; UV Resistant

Appearance: Black; Natural Color

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 21
@Time 10.0 sec
Extruded; ASTM D2240
 23
@Time 10.0 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 508 psiASTM D412
Tensile Stress 73.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 750 %ASTM D412
Tear Strength 112 pliASTM D624
Compression Set 18 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395B
 65 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 - 340 °FHopper, Extrusion
Rear Barrel Temperature 300 - 340 °F
Middle Barrel Temperature 340 - 375 °F
Front Barrel Temperature 390 - 430 °F
Nozzle Temperature 390 - 430 °F
Zone 1 340 - 375 °F
Zone 3 340 - 375 °F
Zone 5 355 - 390 °F
Adapter Temperature 355 - 410 °F
Die Temperature 355 - 410 °F
Melt Temperature 375 - 410 °FInjection
 375 - 430 °FExtrusion
Mold Temperature 50.0 - 120 °FInjection
Drying Temperature 130 - 160 °FInjection
 130 - 160 °FExtrusion
Injection Pressure 750 - 1300 psi
Cushion 0.200 - 0.500 in
Screw Speed 50 - 200 rpmInjection
 100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature194°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTB584 / 311277

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.