MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Entec Enflex® EA3720 Styrenic Block, TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Product Description: 20 Shore A TPE (Styrenic Block Copolymer based) available in black and natural for injection molding and extrusion applications. This grade offers soft/tactile feel and adhesion (overmolding or co-extrusion) to ABS, PC and HIPS/PS

Availability: North America

Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Processability; High Elasticity; Oil Resistant; Ozone Resistant; Recyclable Material; Soft; Solvent Resistant; UV Resistant

Appearance: Black; Natural Color

Processing Method: Extrusion; Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  21
@Time 10.0 sec
21
@Time 0.00278 hour
Extruded; ASTM D2240
 23
@Time 10.0 sec
23
@Time 0.00278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 3.50 MPa508 psiASTM D412
Tensile Stress 0.503 MPa
@Strain 100 %
73.0 psi
@Strain 100 %
ASTM D412
Elongation at Break 750 %750 %ASTM D412
Tear Strength 19.6 kN/m112 pliASTM D624
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395B
 65 %
@Temperature 70.0 °C,
Time 79200 sec
65 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 149 - 171 °C300 - 340 °FHopper, Extrusion
Rear Barrel Temperature 149 - 171 °C300 - 340 °F
Middle Barrel Temperature 171 - 191 °C340 - 375 °F
Front Barrel Temperature 199 - 221 °C390 - 430 °F
Nozzle Temperature 199 - 221 °C390 - 430 °F
Zone 1 171 - 191 °C340 - 375 °F
Zone 3 171 - 191 °C340 - 375 °F
Zone 5 179 - 199 °C355 - 390 °F
Adapter Temperature 179 - 210 °C355 - 410 °F
Die Temperature 179 - 210 °C355 - 410 °F
Melt Temperature 191 - 210 °C375 - 410 °FInjection
 191 - 221 °C375 - 430 °FExtrusion
Mold Temperature 10.0 - 48.9 °C50.0 - 120 °FInjection
Drying Temperature 54.4 - 71.1 °C130 - 160 °FInjection
 54.4 - 71.1 °C130 - 160 °FExtrusion
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 50 - 200 rpm50 - 200 rpmInjection
 100 - 200 rpm100 - 200 rpmExtrusion
 
Descriptive Properties
Dynamic Service Temperature194°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB584 / 311277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.